Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 81.1 °C | 178 °F | Unannealed; ASTM Data |
Americas Styrenics Styron® 678C Polystyrene
(discontinued **) STYRON® 678C general purpose polystyrene resin is a high flow, medium strength resin with good scuff resistance. It is typically used in thin-wall or consumer electronic applications. When used unm.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.1 °C | 178 °F | ASTM D648 |
Ineos T50-400 HDPE T50-400 is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and end-use p.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.1 °C | 178 °F | ASTM D648 |
Ineos T50-500-171 Polyethylene Copolymer This is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and end-use pro.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.1 °C | 178 °F | ASTM D648 |
Ineos T50-500-196 Polyethylene Copolymer This is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and end-use pro.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.1 °C | 178 °F | Unannealed; ASTM D648 |
LyondellBasell Pro-faxâ„¢ RP320N Polypropylene Copolymer Description: Pro-faxâ„¢ RP320N is a barefoot polypropylene random copolymer designed for cast film packaging applications. Cast film made with this resin has exceptional clarity and gloss, as wel.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.1 °C | 178 °F | Unannealed; ASTM D648 |
LyondellBasell Hostacomâ„¢ 6551 Polypropylene Homopolymer Description: Hostacomâ„¢ 6551 conventional melt flow, 1,300 MPa flexural modulus, precolored polypropylene homopolymer has a good combination of strength, stiffness, impact and heat resistance. I.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.1 °C | 178 °F | Unannealed; ASTM D648 |
Dow DS6D21 Polypropylene Random Copolymer Resin OverviewConsistent processabilityHigh clarity and glossComplies with U.S. FDA 21 CFR 177.1520 (c)3.1aDOW DS6D21 Polypropylene Resin is intended for use in case film processes. It is particularly su.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.1 °C | 178 °F | unannealed; molded and tested in accordance with ASTM D 4101; ASTM D648 |
Dow DS6D21 Polypropylene Resin DOW DS6D21 is intended for use in cast film processes. It is particularly suited for applications requiring high clarity.Information provided by DowDow Announced Sale of Global Polypropylene Busine.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.1 °C | 178 °F | ASTM D648 |
Clariant Renol BRU0000BN-182 Nylon 66, Lubricated, Nucleated, Weather Resistant Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.1 °C | 178 °F | ASTM D648 |
Aaron Industries AAROLENE® ARPS 100-3 HIPS Black Injection Grade Polystyrene Compounded Resin, Injection Molding AAROLENE® ARPS 100 Series Polystyrene Compounded ResinFeatures: A high impact Polystyrene, custom colored black, featuring good flow and excellent toughness. |