Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 84.6 °C | 184 °F | ASTM D648 |
Flint Hills 23H2A Random Copolymer Polypropylene Features: Excellent clarity. Product does not contain animal derived components.Applications: Designed for Blow molding and Thermoforming - A replacement for PET, PS and PC high clarity applicatio.. |