Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 99.2 °C | 211 °F | ASTM D648 |
Eastman Tritan GX100 Copolyester Eastman Tritan copolyester GX100's strength, clarity and temperature resistance make it ideal for demanding applications. Extruded Sheet is manufactured with Eastman's Tritan copolyester GX100 resi.. |