Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 99.4 °C
211 °F
Annealed, 0.125 in bars; ASTM D648
PolyOne Edgetek® AS-1000 Acrylonitrile Butadiene Styrene (ABS)  (discontinued **)
Description/Features:UnfilledPolyOne First ChoiceInformation provided by PolyOne Corporation.
Deflection Temperature at 0.46 MPa (66 psi) 99.4 °C
211 °F
Unannealed; ASTM D648
Techmer ES Plastiblend® ABS/PBT 1000
Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 99.4 °C
211 °F
Unannealed; ASTM D648
Techmer ES Plastiblend® ABS/PBT 1500
Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 99.4 °C
211 °F
Unannealed; ASTM D648
Techmer ES Plastiblend® PBT/ABS BK
Availability: North AmericaForms: PelletsAppearance: BlackTPCI# 6722121Information provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 99.4 °C
211 °F
Unannealed; ASTM D648
Styron MAGNUMâ„¢ 375 HH Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection moldingApplications: Automotive interior trim applications requiring low volatile organic compounds (VOC)Information provided by..
Deflection Temperature at 0.46 MPa (66 psi) 99.4 °C
211 °F
Unannealed; ASTM D648
Styron MAGNUMâ„¢ 375 HP Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection molded automotive interior trim applications.Applications: Chrysler-MSDB-191Ford-WSB-M4D690-AGM-GMP.ABS.009Information provided ..
Deflection Temperature at 0.46 MPa (66 psi) 99.4 °C
211 °F
ASTM D648
Plastics Group Polifil® RMC-10 10% Calcium Carbonate-Reinforced Polypropylene, High Impact
Polifil® RMC series compounds are high impact polypropylenes reinforced with fine particle size calcium carbonate. In addition to the highest impact possible, they possess good stiffness, heat agin..
Deflection Temperature at 0.46 MPa (66 psi) 99.2 °C
211 °F
ASTM D648
Eastman Tritan GX100 Copolyester
Eastman Tritan copolyester GX100's strength, clarity and temperature resistance make it ideal for demanding applications. Extruded Sheet is manufactured with Eastman's Tritan copolyester GX100 resi..
Deflection Temperature at 0.46 MPa (66 psi) 99.4 °C
211 °F
Unannealed; ASTM D648
ExxonMobil AP3AW Polypropylene Impact Copolymer
Product Description: A UV stabilized medium impact copolymer resin designed for automotive battery cases.Availability: Asia Pacific Features:Good UV ResistanceHigh StiffnessLow WarpageMedium FlowMe..