Thermal Properties Metric English Comments
UL RTI, Electrical 190 °C

@Thickness 1.57 mm
374 °F

@Thickness 0.0618 in
Solvay Specialty Polymers Veradel® AG-230 Polyethersulfone  (discontinued **)
For superior long-term performance at high temperatures in severe service environments. It offers especially good toughness, hydrolytic stability, chemical resistance, plus FDA and USDA compliance.N..
UL RTI, Electrical 190 °C
374 °F
50% decrease of tensile strength after 20000h; 746B
BASF Ultrason E 1010 PES
Ultrason E 1010 is an unreinforced, low viscosity injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability.
UL RTI, Electrical 190 °C
374 °F
50% decrease of tensile strength after 20000h; 746B
BASF Ultrason E 2010 PES
Ultrason E 2010 is an unreinforced, medium viscosity standard injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req..