Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 190 °C @Thickness 1.57 mm |
374 °F @Thickness 0.0618 in |
|
Solvay Specialty Polymers Veradel® AG-230 Polyethersulfone
(discontinued **) For superior long-term performance at high temperatures in severe service environments. It offers especially good toughness, hydrolytic stability, chemical resistance, plus FDA and USDA compliance.N.. |
|||
UL RTI, Electrical | 190 °C | 374 °F | 50% decrease of tensile strength after 20000h; 746B |
BASF Ultrason E 1010 PES Ultrason E 1010 is an unreinforced, low viscosity injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. |
|||
UL RTI, Electrical | 190 °C | 374 °F | 50% decrease of tensile strength after 20000h; 746B |
BASF Ultrason E 2010 PES Ultrason E 2010 is an unreinforced, medium viscosity standard injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req.. |