Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 130 - 240 °C | 266 - 464 °F | Average value: 191 °C Grade Count:5 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
UL RTI, Electrical | 220 - 240 °C | 428 - 464 °F | Average value: 228 °C Grade Count:5 |
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini.. |
|||
UL RTI, Electrical | 220 - 240 °C | 428 - 464 °F | UL 746B |
Solvay Specialty Polymers Ryton® R-7-121NA Polyphenylene Sulfide Resin
(Unverified Data**) Ryton® R-7-121NA is an advanced glass/mineral filled polyphenylene sulfide compound developed to provide good mechanical strength with good flow and low maintenance molding using conventional moldi.. |