Polymer Property : UL RTI, Electrical = 266 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
UL RTI, Electrical 130 °C
266 °F
UL 746C
Premix Premi-Glas® 1200H-10 Fiberglass Reinforced Thermoset SMC
Premi-Glas® 1200H-10 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:G..
UL RTI, Electrical 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 101R PC (Asia Pacific)
Nonhalogenated. 7.0 MFR, for thicker sections without sinks. Internal mold release.
UL RTI, Electrical 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 121 PC
UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small intricate parts.
UL RTI, Electrical 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 201 PC
7.0 MFR, for thicker sections without sinks. Improved flame retardance.
UL RTI, Electrical 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 201 PC (Asia Pacific)
7.0 MFR, for thicker sections without sinks. Improved flame retardance.
UL RTI, Electrical 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 203 PC (Asia Pacific)
7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting.
UL RTI, Electrical 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 241 PC (Asia Pacific)
10.5 MFR. Improved flame retardance.
UL RTI, Electrical 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 244RF PC (Asia Pacific)
LEXAN 244RF resin grade is a medium viscosity multi purpose product with improved flame resistance and release properties. It is also FDA food contact compliant available in limited colors.
UL RTI, Electrical 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 505R PC
Lexan* 505R Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. Lexan 505R contains non-chlorinated, non-brominated flame retardant systems with UL-94 V0 rating at 1.5mm...
UL RTI, Electrical 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® EXL1443T PC Copolymer
Lexan* EXL1443T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers excellent low temperature (-30 C) ductility in co..
UL RTI, Electrical 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char..
UL RTI, Electrical 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer
Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA.
UL RTI, Electrical 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® FXE101R PC (Europe-Africa-Middle East)
Transparent PC. ILLUMINATE special effects (fluorescent/edge glow colors). For thicker sections without sinks. Internal mold release.This data was supplied by SABIC-IP for the Europe-Africa-Middl..
UL RTI, Electrical 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® LUX2010T_ PC (Europe-Africa-Middle East)
Global grade. LEXAN LUX2010T is an injection moulding grade especially designed for manufacturing optical parts requiring excellent flow properties combined with very high transmission and color sta..
UL RTI, Electrical 130 °C
266 °F
UL 746B
SABIC Innovative Plastics LNP KONDUIT OX10324 PPS (Asia Pacific)
Thermally conductive mineral filled PPS FR compound, with through-plane and in-plane thermal conductivity of 3.5 W/(m*K) and 15 W/(m*K) respectively, conforming to ASTM E 1461 test standard.
UL RTI, Electrical 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 144R PC (Europe-Africa-Middle East)
Medium viscosity, multi purpose polycarbonate resin with added release agent. Food contact approved in limited colors. Effective January 15th, 2007 this grade will no longer be supported with bioc..
UL RTI, Electrical 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 3412ECR PC (Europe-Africa-Middle East)
Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v..
UL RTI, Electrical 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 925 PC (Europe-Africa-Middle East)
Lexan* 925A Polycarbonate (PC) resin is a non-filled, injection moldable grade of non-chlorinated, non-brominated flame retardant systems that has an UL-94 V0 rating. Lexan 925A is available in tran..
UL RTI, Electrical 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 925AU PC
Lexan* 925AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing addit..
UL RTI, Electrical 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 925AU PC (Asia Pacific)
Lexan* 925AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing addit..
UL RTI, Electrical 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 955A PC
Lexan* 955A Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating. Lexan 955A resin is available in tran..
UL RTI, Electrical 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® EXL1414T PC Copolymer (Asia Pacific)
Lexan* EXL1414T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo..
UL RTI, Electrical 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® EXL1414T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1414T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo..
UL RTI, Electrical 130 °C
266 °F
Glastic Laminates/Shapes 2015 Fiberglass-Reinforced Polyester Standoff Insulator
Data provided by Glastic Corporation.Molded from UL recognized molding compound. Moisture and heat resistance of Glastic Insulators are higher than those of conventional plastic insulators.
UL RTI, Electrical 130 °C
266 °F
Glastic Laminates/Shapes 2035-1 Fiberglass-Reinforced Polyester Standoff Insulator
Data provided by Glastic Corporation.Molded from UL recognized molding compound. Moisture and heat resistance of Glastic Insulators are higher than those of conventional plastic insulators.
UL RTI, Electrical 130 °C
266 °F
UL temperature Index, UL 746B
Sumitomo Bakelite North America 52-01 Short-Glass Reinforced Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG.Inf..
UL RTI, Electrical 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Valox® IQNH4550 PBT (Europe-Africa-Middle East)
Valox* iQNH4550 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% based on EPEAT..
UL RTI, Electrical 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 103R PC
UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV Stabilized for outdoor and lighting. Internal mold release...
UL RTI, Electrical 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 940 PC
Opaque colors, medium viscosity, superior flame retardance.
UL RTI, Electrical 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® HP4NR PC
Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no m..