Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 115 °C | 239 °F | UL 746 |
PolyOne Maxxam™ FR PP 402 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
UL RTI, Mechanical without Impact | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C2100 PC+ABS (Asia Pacific) CYCOLOY C2100 is a flame retardant blend, specifically developed to meet the stringent requirements of mains current carrying applications. CYCOLOY C2100 combines |
|||
UL RTI, Mechanical without Impact | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C2100 PC+ABS (Europe-Africa-Middle East) CYCOLOY C2100 is a flame retardant blend, specifically developed to meet the stringent requirements of mains current carrying applications. CYCOLOY C2100 combinesThis data was supplied by SABIC-IP f.. |
|||
UL RTI, Mechanical without Impact | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics Lexan® 303 PC (Asia Pacific) Clear, high viscosity material designed to service severe environments of HID lighting.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
UL RTI, Mechanical without Impact | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics Lexan® ML3019 PC (Europe-Africa-Middle East) LEXAN ML3019 is a medium viscosity, 10% glass reinforced, flame retardant grade, especially designed for applications like industrial enclosures and fuse boxes requiring a low knock-out strength for.. |
|||
UL RTI, Mechanical without Impact | 115 °C | 239 °F | 0.118 in; UL 746 |
LyondellBasell Hifaxâ„¢ AA36H Polypropylene Homopolymer Description: Hifaxâ„¢ AA36H conventional melt flow, 1,400 MPa flexural modulus, UL 94 V-2 flame retardant polypropylene homopolymer resin has an excellent combination of properties and processabi.. |
|||
UL RTI, Mechanical without Impact | 115 °C | 239 °F | 0.118 in; UL 746 |
LyondellBasell Hifaxâ„¢ AA56H Polypropylene Homopolymer Description: Hifaxâ„¢ AA56H medium high melt flow, 1,400 MPa flexural modulus, UL 94 V-2 flame retardant polypropylene homopolymer resin has an excellent combination of properties and processabil.. |
|||
UL RTI, Mechanical without Impact | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics NORYL V0150B PPE+HIPS Noryl* V0150B is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm a.. |
|||
UL RTI, Mechanical without Impact | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics NORYL V0150B PPE+HIPS (Asia Pacific) Noryl* V0150B is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm a.. |
|||
UL RTI, Mechanical without Impact | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics NORYL V0150B PPE+HIPS (Europe-Africa-Middle East) Noryl* V0150B is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm a.. |
|||
UL RTI, Mechanical without Impact | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
UL RTI, Mechanical without Impact | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Asia Pacific) Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
UL RTI, Mechanical without Impact | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Europe-Africa-Middle East) Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
UL RTI, Mechanical without Impact | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics ULTEM ATX100 PEI+PCE Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. |
|||
UL RTI, Mechanical without Impact | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics ULTEM ATX100 PEI+PCE (Asia Pacific) Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. |
|||
UL RTI, Mechanical without Impact | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics Ultem ATX100F PEI+PCE Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. US FDA Food Contact Compliant.This data was supplied by SABIC-IP for the Americas region. |
|||
UL RTI, Mechanical without Impact | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics Ultem ATX100F PEI+PCE (Asia Pacific) Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. US FDA Food Contact Compliant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
UL RTI, Mechanical without Impact | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics Ultem ATX100R PEI+PCE Higher impact, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 HB listing.This data was supplied by SABIC-IP for the Americas region. |
|||
UL RTI, Mechanical without Impact | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics Ultem ATX100R PEI+PCE (Asia Pacific) Higher impact, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 HB listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
UL RTI, Mechanical without Impact | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics ULTEM ATX200F PEI+PCE High flow Polyetherimide blend. ECO Conforming, UL94 V0 Listing. US FDA Food Contact compliant. |
|||
UL RTI, Mechanical without Impact | 115 °C | 239 °F | UL746 |
Techmer ES HiFill FR® PA6 GF33 FR HS L 33% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and Lu.. |
|||
UL RTI, Mechanical without Impact | 115 °C | 239 °F | UL746 |
Techmer ES HiFill FR® PA6 GF33 FR HS L BK065 33% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and Lu.. |
|||
UL RTI, Mechanical without Impact | 115 °C | 239 °F | UL746 |
Techmer ES HiFill FR® PA6 GF33 FR HS L GY300 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer, UV Stabilizer and LubricantFeatures: Flame Retardant, Heat St.. |
|||
UL RTI, Mechanical without Impact | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics LNP THERMOCOMP UF007AS PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UF007AS is a compound based on Polyphthalamide resin containing Glass Fiber. Added features include Heat Stabilized . |
|||
UL RTI, Mechanical without Impact | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics NORYL LTA1350 PPE+PS Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
UL RTI, Mechanical without Impact | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics ULTEM ATX200 PEI+PCE High flow Polyetherimide blend. ECO Conforming, UL94 V0 Listing. |
|||
UL RTI, Mechanical without Impact | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics ULTEM ATX200 PEI+PCE (Asia Pacific) High flow Polyetherimide blend. ECO Conforming, UL94 V0 Listing. |
|||
UL RTI, Mechanical without Impact | 115 °C | 239 °F | |
Eurostar Starflam AFR200Y PA66, Flame Retardant, Injection Molding Staramide AFR200Y is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 2.50 mm |
239 °F @Thickness 0.0984 in |
746B |
BASF Ultramid® 8232G HS FR 25% Glass Fiber Fire Retardant PA6 (Conditioned) Description: Ultramid 8232G HS FR is a 25% glass fiber reinforced, heat stabilized, flame retardant PA6 injection molding compound exhibiting excellent melt stability characteristics. It combines fl.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 1.50 mm |
239 °F @Thickness 0.0591 in |
746B |
BASF Ultramid® 8232G HS FR 25% Glass Fiber Fire Retardant PA6 (Dry) Description: Ultramid 8232G HS FR is a 25% glass fiber reinforced, heat stabilized, flame retardant PA6 injection molding compound exhibiting excellent melt stability characteristics. It combines fl.. |