Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Lexan® FL920 PC (Europe-Africa-Middle East) LEXAN FL920 is a foamable grade of LEXAN polycarbonate, containing 20% glass-fibre is designed of applications where superior flexural and tensile charasterics are required. LEXAN FL920 also offers .. |
|||
UL RTI, Mechanical without Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Lexan® FL930 PC Various weight reductions at 0.250"" (6.35 mm) wall, 30% GR. Superior flex strength/modulus, good tensile strength. V-0/5VA at 0.250"" (6.35 mm). |
|||
UL RTI, Mechanical without Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Lexan® FL930 PC (Asia Pacific) Various weight reductions at 0.250"" (6.35 mm) wall, 30% GR. Superior flex strength/modulus, good tensile strength. V-0/5VA at 0.250"" (6.35 mm). |
|||
UL RTI, Mechanical without Impact | 110 °C @Thickness 6.00 mm |
230 °F @Thickness 0.236 in |
|
Covestro Makrolon® SF-800 Polycarbonate, Structural Foam
(discontinued **) Properties based on foam density of 0.90 g/cc.Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially.. |
|||
UL RTI, Mechanical without Impact | 110 °C | 230 °F | UL746B |
Idemitsu Kosan Xarec® EA 543 SPS, 40% Glass Filled |
|||
UL RTI, Mechanical without Impact | 110 °C | 230 °F | UL746B |
Idemitsu Kosan Xarec® WA 212 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled, Impact Modified. Used in Automotive and Industrial applications. |
|||
UL RTI, Mechanical without Impact | 110 °C | 230 °F | UL746B |
Idemitsu Kosan Xarec® WA 552 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled/Impact Modified. Used in Automotive and Industrial applications. NSF and medical approval ISO 10993 |
|||
UL RTI, Mechanical without Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL PX9406 PPE+PS Nonbrominated, nonchlorinated, flame retarded. Improved productivity and reliability. 252F HDT. UL94 V-0 rated. Electrical applications. |
|||
UL RTI, Mechanical without Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL PX9406 PPE+PS (Asia Pacific) Nonbrominated, nonchlorinated, flame retarded. Improved productivity and reliability. 252F HDT. UL94 V-0 rated. Electrical applications. |
|||
UL RTI, Mechanical without Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL SE1GFN1 PPE+HIPS (Europe-Africa-Middle East) Noryl* SE1GFN1 is a 10% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non.. |
|||
UL RTI, Mechanical without Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL SE1GFN1 PPE+PS PPE+PS blend. 10% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 listing. RTI 110/105/110. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
UL RTI, Mechanical without Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL SE1GFN1 PPE+PS (Asia Pacific) 10% GR. UL94 V-1 rated. Halogen free flame retardant. Typical applications are TV chassis, deflection yokes and connectors. |
|||
UL RTI, Mechanical without Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL SE1GFN2 PPE+HIPS (Europe-Africa-Middle East) Noryl* SE1GFN2 is a 20% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non.. |
|||
UL RTI, Mechanical without Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL SE1GFN3 PPE+PS (Asia Pacific) GR 30%. 275F (135C) DTUL. UL94 V-1 rated. Halogen free flame retardant. For electrical construction market. |
|||
UL RTI, Mechanical without Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Valox® 865 PBT+PET (Asia Pacific) 30% GR PBTP, UL94 V-0 rated. Non-blooming flame retardant. Improved surface appearance. Same application areas as for VALOX 855. |
|||
UL RTI, Mechanical without Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Asia Pacific) Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
UL RTI, Mechanical without Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Europe-Africa-Middle East) Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
UL RTI, Mechanical without Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to.. |
|||
UL RTI, Mechanical without Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
UL RTI, Mechanical without Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
UL RTI, Mechanical without Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
UL RTI, Mechanical without Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Asia Pacific) Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
UL RTI, Mechanical without Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_PX5379 PPE+HIPS (Europe-Africa-Middle East) LNP* Thermocomp* Noryl_PX5379 compound is a 10% GR. UL94 V-1 rated. Halogen free flame retardant. Typical applications are TV chassis, deflection yokes and connectors. |
|||
UL RTI, Mechanical without Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics LNP Verton RV00AESM PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00AESM is a compound based on PA66 resin containing Long Glass Fiber. Added features include: Easy Moldin, Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Mid.. |
|||
UL RTI, Mechanical without Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics LNP VERTON RV00AESS PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00AESS is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding, Heat Stabilized. |
|||
UL RTI, Mechanical without Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics LNP VERTON RV00AEX5 PA6.6 (Europe-Africa-Middle East) LNP* VERTON* Is a compound based on PA66 resin containing Long Glass Fiber. Added features include: Easy Molding, Heat Stabilized. |
|||
UL RTI, Mechanical without Impact | 110 °C | 230 °F | |
Aclo Accuguard Polypropylene HP1362V2CSL Homopolymer Flame Retardant Copper Stabilized |
|||
UL RTI, Mechanical without Impact | 110 °C | 230 °F | |
Aclo Accuguard Polypropylene HP1369V2CSL Homopolymer Flame Retardant Copper Stabilized |
|||
UL RTI, Mechanical without Impact | 110 - 130 °C | 230 - 266 °F | Average value: 122 °C Grade Count:16 |
Overview of materials for Nylon 46, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values .. |
|||
UL RTI, Mechanical without Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics LNP VERTON RV00ASXS PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00ASXS is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Heat Stabilized |