Material Notes:
PPE+PS blend. 10% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 listing. RTI 110/105/110. Dielectric strength. Dimensional stability. Suitable for E/E applications.
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Water Absorption 0.070 %

@Time 86400 sec
0.070 %

@Time 24.0 hour
ASTM D570
Moisture Absorption at Equilibrium 0.22 %
0.22 %
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm

@Thickness 3.20 mm
0.0030 - 0.0050 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Hardness, Rockwell L 104
104
ASTM D785
Tensile Strength at Break 74.0 MPa
10700 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 5.0 %
5.0 %
Type I, 5 mm/min; ASTM D638
Flexural Strength 119 MPa
17300 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 3.99 GPa
579 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
0.690 J/cm

@Temperature -40.0 °C
1.29 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 131 °C

@Thickness 6.40 mm
268 °F

@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 147 °C
297 °F
Rate B/50; ASTM D1525
UL RTI, Electrical 110 °C
230 °F
UL 746B
UL RTI, Mechanical with Impact 105 °C
221 °F
UL 746B
UL RTI, Mechanical without Impact 110 °C
230 °F
UL 746B
Flammability, UL94 V-1

@Thickness 1.47 mm
V-1

@Thickness 0.0579 in
UL 94
Oxygen Index 33.9 %
33.9 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Dielectric Constant 3.0

@Frequency 1.00e+6 Hz
3.0

@Frequency 1.00e+6 Hz
ASTM D150
3.0

@Frequency 50.0 - 60.0 Hz
3.0

@Frequency 50.0 - 60.0 Hz
ASTM D150
Dissipation Factor 0.0016

@Frequency 1.00e+6 Hz
0.0016

@Frequency 1.00e+6 Hz
ASTM D150
0.0017

@Frequency 50.0 - 60.0 Hz
0.0017

@Frequency 50.0 - 60.0 Hz
ASTM D150
Comparative Tracking Index 250 - 400 V
250 - 400 V
UL 746A
Hot Wire Ignition, HWI 60 - 120 sec
60 - 120 sec
UL 746A
High Amp Arc Ignition, HAI 30 - 60 arcs
30 - 60 arcs
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/min
>= 5.91 in/min
UL 746A