Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics Cycolac® GPM5500 ABS (Europe-Africa-Middle East) CYCOLAC GPM5500 is a multi purpose injection moulding grade, providing a favourable balance of engineering properties. CYCOLAC GPM5500 has a wide processing window. It is recommended for application.. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 1.70 mm |
149 °F @Thickness 0.0669 in |
UL 746 |
Polymer Resources PPX-FRG20 Modified-PPO, V-1 Flame Retardant, 20% Glass Reinforced Modified-Polyphenylene Oxide, V-1 Flame Retardant, 20% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu.. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PPX-GP1-[color]-EN Modified-PPO, Extrusion Grade Modified-Polyphenylene Oxide, Extrusion Grade, 265F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Extrusion Notes: All physical, mechanical and thermal testing conduc.. |
|||
UL RTI, Mechanical without Impact | 65.0 - 140 °C | 149 - 284 °F | Average value: 98.0 °C Grade Count:4 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness >=0.700 mm |
149 °F @Thickness >=0.0276 in |
|
LG Chemical LUMID GP1000B(W) PA66, General Purpose, Low Viscosity Feature: Injection Molding, PA66, General Purpose, Low ViscosityApplication: Buckles, Chair NobCAS No. 32131-17-2Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness >=0.750 mm |
149 °F @Thickness >=0.0295 in |
|
LG Chemical LUMID GP2300A(W) PA6+GF30%, General Purpose Feature: Injection Molding, PA6+GF30%, General PurposeApplication: Automotive (Side Mirror Base Plate)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness >=0.750 mm |
149 °F @Thickness >=0.0295 in |
|
LG Chemical LUMID GP2430A(W) PA6+GF43%, General Purpose Feature: Injection Molding, PA6+GF43%, General PurposeApplication: Automotive (Air Intake Manifold, Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness >=1.50 mm |
149 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOL HG3100 PP+MF10%, High Gloss Description: Injection Molding, PP+MF10%, High GlossApplication: Electrical & Electronic PartsCAS: 9003-07-0 and 7727-43-7Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness >=1.50 mm |
149 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOL GP3402 PP+MF40% Description: Injection Molding, PP+MF40%, General PurposeApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics LNP THERMOCOMP PF006S PA 6 (Europe-Africa-Middle East) Heat stabilized, 30% glass fibre reinforced Polyamide 6 injection moulding resin. |
|||
UL RTI, Mechanical without Impact | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics LNP Thermocomp RF0069 PA 66 (Europe-Africa-Middle East) Flame retarded, 30% glass fibre reinforced Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
UL RTI, Mechanical without Impact | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics Noryl N1251 PPE+PS ECO-FLO(tm). ECO conforming, non-halogen flame retardant PPE+PS. High flow. Electrical and Business Equipment applications.This data was supplied by SABIC-IP for the Americas region. |
|||
UL RTI, Mechanical without Impact | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Europe-Africa-Middle East) Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity... |
|||
UL RTI, Mechanical without Impact | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics LNP Thermocomp R1000HI620 PA 66 (Europe-Africa-Middle East) Impact modified Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 0.749 mm |
149 °F @Thickness 0.0295 in |
UL 746 |
Teknor Apex Chemlon® 125-15 MGH Nylon 66, 25% Mineral Reinforced, 15% Glass Fiber Reinforced Notes: 25% Mineral - 15% Glass; Excellent stiffness and strength, especially at high temperatures, with improved warpage control over glass reinforced products; FMVSS Flammability: Passes, FMVSS 302.. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 0.780 mm |
149 °F @Thickness 0.0307 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1006 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1006 is a 20% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 0.780 mm |
149 °F @Thickness 0.0307 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1006S Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1006S is a 20% talc filled homopolymer polypropylene compound formulated with an internal mold release. Information provided by A. Schulman. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 0.780 mm |
149 °F @Thickness 0.0307 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1006 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1006 is a 20% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 0.780 mm |
149 °F @Thickness 0.0307 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1006 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1006 is a 20% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
UL RTI, Mechanical without Impact | 65.0 °C | 149 °F | |
Eurostar Staramide B40 PA6, Extrusion Staramide B40 is High Viscosity, Unreinforced Polyamide 6, Extrusion ResinInformation provided by Eurostar. |
|||
UL RTI, Mechanical without Impact | 65.0 °C | 149 °F | |
Eurostar Staramide BG7HU PA6, 35% Glass Fiber Filled, Heat and UV Stabilized, Injection Molded Staramide BG7H is a Heat and UV Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
UL RTI, Mechanical without Impact | 65.0 °C | 149 °F | |
Eurostar Starflam AFR200B PA66, Flame Retardant, Injection Molding Staramide AFR200B is an Unfilled, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
UL RTI, Mechanical without Impact | 65.0 °C | 149 °F | |
Eurostar Starflam BFR460B1 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR460B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 1.60 mm |
149 °F @Thickness 0.0630 in |
|
Eurostar Starflam PK0022E PA6, 10% Mineral Filled, Injection Molded PK0022E is a Halogen Free and Phosphorous Free, Mineral Filed, Polyamide 6 Injection Molding (also known as PM3620Z22 or PA 10E6 U9 Z22)Information provided by Polymer Technology & Services, the Nor.. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
|
Eurostar Starflam PW0042E PA6, 20% Mineral Filled, Injection Molded PW0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Mineral Reinforced, Polyamide 6 Injection MoldingInformation provided by Polymer Technology & Services, the North American exclus.. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness 0.800 mm |
149 °F @Thickness 0.0315 in |
|
Eurostar Starflam PK0052E PA6, 25% Mineral Filled, Injection Molded PK0052E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Mineral Filed, Polyamide 6 Injection Molding (also known as PM3520Z222 or PA 25E6 U9 Z22)Information provided by Polymer Technolo.. |
|||
UL RTI, Mechanical without Impact | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics NORYL FP5140HF PPE+PS Noryl*FP5140HF is an unfilled, injection moldable modified polyphenylene ether resin with an ISO306 Vicat B/120 of 100 deg C. Designed for good dimensional stability and high flow, this resin also u.. |
|||
UL RTI, Mechanical without Impact | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Europe-Africa-Middle East) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
UL RTI, Mechanical without Impact | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics NORYL RN0611 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0611 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen.. |
|||
UL RTI, Mechanical without Impact | 65.0 °C @Thickness >=0.750 mm |
149 °F @Thickness >=0.0295 in |
|
LG Chemical LUMID GP3300A(W) PA6+MF30%, General Purpose Feature: Injection Molding, PA6+MF30%, General PurposeApplication: Automotive (Battery Pack Housing)Information provided by LG Chemical |