Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 85.0 °C | 185 °F | UL 746 |
PolyOne Geon™ Vinyl Rigid Molding M3500 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
UL RTI, Mechanical without Impact | 85.0 °C | 185 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications. |
|||
UL RTI, Mechanical without Impact | 85.0 °C | 185 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications. |
|||
UL RTI, Mechanical without Impact | 85.0 °C | 185 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C2950HF PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced impact and heat properties plus improved flow for various applications. |
|||
UL RTI, Mechanical without Impact | 85.0 °C | 185 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C2951 PC+ABS (Asia Pacific) CYCOLOY C2951 is a flame retardant PC+ABS free from chlorinated or brominated flame retardant additives. High heat resistance is offered for demanding electrical applications, whilst maintaining exc.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C | 185 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C6200 PC+ABS (Asia Pacific) Non-chlorinated, nombrominated flame retardant PC/ABS offering balanced heat, flow and impact to meet various application needs. |
|||
UL RTI, Mechanical without Impact | 85.0 °C | 185 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C6200 PC+ABS (Europe-Africa-Middle East) CYCOLOY C6200 is a non-chlorinated, nombrominated flame retardant PC/ABS offering balanced heat, flow and impact to meet various application needs. C6200 has improved processing window and edge crac.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C | 185 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C | 185 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C | 185 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C | 185 °F | Ul746B |
Parker Chomerics PREMIER™ A220-HT EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
UL RTI, Mechanical without Impact | 85.0 °C | 185 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C6200 PC+ABS Non-chlorinated, nombrominated flame retardant PC/ABS offering balanced heat, flow and impact to meet various application needs. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 1.57 mm |
185 °F @Thickness 0.0618 in |
|
Covestro Bayblend® 2153 Polycarbonate + ABS Blend, General Purpose
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 1.57 mm |
185 °F @Thickness 0.0618 in |
|
Covestro Bayblend® 2773 Polycarbonate + ABS Blend, Automotive
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 1.57 mm |
185 °F @Thickness 0.0618 in |
Bayer provisional value |
Covestro Bayblend® KU2-1500 Polycarbonate + ABS Blend, Extrusion/Blow-Molding
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C | 185 °F | |
Covestro Bayblend® FR 2000 Polycarbonate/ABS Blend
(discontinued **) Easy-flowing FR grade. Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, optimized processability.Applications: Housings for office equipment, electrical engin.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 0.710 mm |
185 °F @Thickness 0.0280 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 101L BKB080 Nylon 66
(Unverified Data**) Zytel® 101L BKB080 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 85.0 °C | 185 °F | |
LG Chemical LUPOY GN5001RFP PC/ABS, Halogen Free Flame Retardant, Heat Resistance Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, General PurposeApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Ch.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C | 185 °F | |
LG Chemical LUPOY GN5001RFT PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Good FlowApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C | 185 °F | |
Samsung Cheil Industries Infino® GC-1017 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
UL RTI, Mechanical without Impact | 85.0 °C | 185 °F | |
Samsung Cheil Industries Infino® NH-1017D PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
UL RTI, Mechanical without Impact | 85.0 °C | 185 °F | |
Samsung Cheil Industries Infino® NH-1017D PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
UL RTI, Mechanical without Impact | 85.0 °C | 185 °F | UL 746B |
SABIC Innovative Plastics Noryl PX1115 PPE+HIPS (Europe-Africa-Middle East) NORYL PX1115 is an unfilled, flame retardant material with a Vicat B/120 of 140°C according ISO 306. NORYL PX1115 is V1 at 1.2 mm according UL94 and halogen free according VDE/DIN 472 part 815.Th.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C | 185 °F | |
Samsung Cheil Industries Infino® GC-1017 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
UL RTI, Mechanical without Impact | 85.0 °C | 185 °F | |
Covestro Bayblend® FR 110 Polycarbonate/ABS Blend Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, good light stability.Applications: Housings for business machines.Information provided by Bayer.As of 1 Septe.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 0.810 mm |
185 °F @Thickness 0.0319 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® ST801A NC010A Nylon 66
(Unverified Data**) Zytel® ST801A NC010A is a Super Tough, high performance, polyamide 66 resin. It is partially UV stabilized and when appropriately colored offers limited protection to indirect sunlight exposure.Inf.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 0.750 mm |
185 °F @Thickness 0.0295 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® ST801AW BK195 Nylon 66
(Unverified Data**) Zytel® ST801AW BK195 is a Super Tough, weatherable, easy flow and processing friendly, black polyamide 66 resin for injection molding. It offers the best resistance to outdoor exposure.Information.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 0.710 mm |
185 °F @Thickness 0.0280 in |
UL 746B |
Ascend Performance Materials Vydyne® 22WSP Nylon 66, Weather Resistant, DAM Vydyne® 25WSP is a black, weather resistant injection molding grade Nylon 66 resin. These resins offer a well-balanced combination of engineering properties characterized by high strength, rigidity.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C | 185 °F | UL 746B |
SABIC Innovative Plastics Noryl FN215D PPE+HIPS (Europe-Africa-Middle East) NORYL FN215 is a Noryl Engineering structural foam grade fulfilling a wide range of application requirement. Moulded with the recommended blowing agents, this material provides all the performance r.. |