Pour Point -32.8 °C
-27.0 °F
ASTM D5950/D97
ExxonMobil Exterex™ P81 Synthetic Fluid
Product Description: Esterex™ Phthalate Esters are API category Group V fluids. Esterex™ Phthalate Esters have excellent lower-temperature properties, good lubricating properties and low volatilit..
Pour Point -32.8 °C
-27.0 °F
ASTM D5950/D97
ExxonMobil Exterex™ TM111 Synthetic Fluid
Product Description: Esterex™ Tirmellitate Esters are API category Group V fluids. These esters have excellent low-temperature properties, good lubricating properties and low volatilities. Esterex™..
Pour Point -32.8 °C
-27.0 °F
ASTM D5950/D97
ExxonMobil SpectraSyn Elite™ 150 Metallocene Polyalphaolefin (mPAO) Fluid
Product Description: SpectraSyn ™ metallocene Polyalphaolefin (mPAO) basestock is an advanced high viscosity (Hi-Vis) Polyalphaolefin (PAO). SpectraSyn ™ mPAO utilized metallocene catalyst technol..
Pour Point -32.8 °C
-27.0 °F
ConocoPhillips Conoco® El Mar® Grade 30 Mid Ash Supreme Oil
Conoco® El Mar Mid Ash Supreme is a premium quality, mid-ash, dispersant-detergent gas engine oil designed for use in naturally aspirated and moderately to highly turbocharged 4-stroke cycle natura..
Pour Point -32.8 °C
-27.0 °F
ConocoPhillips El Mar® Grade 15W-40 Geo Oil
Description: Conoco El Mar® Geo Oil is a high-quality, rust- and oxidation-inhibited, nondetergent, ashless gas engine oil. It is formulated with high viscosity index paraffinic base oils blended w..
Pour Point -32.8 °C
-27.0 °F
ConocoPhillips Hydroclear® 20W-50 High Performance Motor Oil SAE 20W-50
Description: Conoco Hydroclear High Performance Motor Oil SAE 20W-50, formulated with premium base stocks, lubricates gasoline engines that operate under severe driving conditions. It is particularl..
Pour Point -32.8 °C
-27.0 °F
ConocoPhillips Hydroclear® 30 Super All Season and Super Motor Oil
Description: Conoco Hydroclear Super All Season and Super Motor Oils, formulated with premium base stocks, lubricate domestic and imported passenger cars, sport-utility vehicles, light-duty trucks, ..
Pour Point -32.8 °C
-27.0 °F
ASTM D5950/D97
ExxonMobil SpectraSyn Ultra™ 150 High VI Polyalphaolefin (PAO) Fluid
Product Description: SpectraSyn Ultra™ High VI Polyalphaolefin (PAO) have high viscosity indices, low pour points, low traction, good air release, and low foaming tendency. The extremely high visco..
Pour Point -32.8 °C
-27.0 °F
ConocoPhillips Hydroclear® 40 Super All Season and Super Motor Oil
Description: Conoco Hydroclear Super All Season and Super Motor Oils, formulated with premium base stocks, lubricate domestic and imported passenger cars, sport-utility vehicles, light-duty trucks, ..