Material Notes:
Product Description: Esterex™ Tirmellitate Esters are API category Group V fluids. These esters have excellent low-temperature properties, good lubricating properties and low volatilities. Esterex™ Trimellitate Esters can be used as sole basestocks or blendstocks with other synthetic fluids in many engine and industrial lubricant applications.Appearance: Bright & ClearAvailability: Asia Pacific, Central America, North America and South AmericaInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.978 g/cc

@Temperature 15.6 °C
0.0353 lb/in³

@Temperature 60.1 °F
ASTM D4052
Viscosity Measurement 81
81
Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 124 cSt
124 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 11.9 cSt
11.9 cSt
ASTM D445
Evaporation Loss 1.0 %

@Temperature 205 °C,
Time 23400 sec
1.0 %

@Temperature 401 °F,
Time 6.50 hour
ASTM D972
Thermal Properties Metric English Comments
Pour Point -32.8 °C
-27.0 °F
ASTM D5950/D97
Flash Point 240 °C
464 °F
PMCC; ASTM D92
274 °C
525 °F
COC; ASTM D92
Optical Properties Metric English Comments
Refractive Index 1.4845
1.4845
ASTM D1218
Chemical Properties Metric English Comments
Acid Value <= 0.16
<= 0.16
[mg KOH/g]; ASTM D974 (mod)
Descriptive Properties Value Comments
Aniline Point 16.5°F
ASTM D611
Biodegradation <1%
OECD 301F
Color <0.5
ASTM D1500
Composition Water
<1000 ppm, ASTM D6304 (mod)
Density Correction Factor 0.000733 (g/cc)/°C
ASTM D1250
Elastomer Compatibility -0.005
Nitrile Tensile Strength Change, ASTM D471
0.023
Fluoroelastomer Volume Change, ASTM D471
-0.03
Fluoroelastomer Hardness Change, ASTM D471
0.092
Fluoroelastomer Elongation Change, ASTM D471
-0.1
Nitrile Hardness Change, ASTM D471
0.145
Nitrile Volume Change, ASTM D471
0.151
Polyacrylate Elongation Change, ASTM D471
-0.16
Polyacrylate Hardness Change, ASTM D471
0.181
Polyacrylate Volume Change, ASTM D471
-0.188
Nitrile Elongation Change, ASTM D471
-0.207
Fluoroelastomer Tensile Strength Change, ASTM D471
-0.243
Polyacrylate Tensile Strength Change, ASTM D471
Fire point 576°F
COC, ASTM D92
Hydrolytic Stability, TAN Change 0.01 mg KOH/g
ASTM D2619
Kauri-Butanol Value 35
ASTM D1133
Noack Volatility 0.014
ASTM D5800/DIN 51581
RPVOT >1210 min
With AO, ASTM D2272
310 min
Neat, ASTM D2272