Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -57.2 °C | -71.0 °F | ASTM D5950/D97 |
ExxonMobil Exterex™ A51 Synthetic Fluid Product Description: Esterex™ Adipate Esters are API category Group V fluids. These esters have excellent low-temperature properties, high viscosity indices, good lubricating properties and low vol.. |
|||
Pour Point | -57.2 °C | -71.0 °F | ASTM D5950/D97 |
ExxonMobil SpectraSyn™ 2C Polyalphaolefin (PAO) Fluid Product Description: SpectraSyn™ Low Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties, low volatility, and improved thermal stability. SpectraSyn™ Low Viscosity (PAO) .. |
|||
Pour Point | -57.2 °C | -71.0 °F | ASTM D5950/D97 |
ExxonMobil SpectraSyn™ 5 Polyalphaolefin (PAO) Fluid Product Description: SpectraSyn™ Low Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties, low volatility, and improved thermal stability. SpectraSyn™ Low Viscosity (PAO) .. |
|||
Pour Point | -57.2 °C | -71.0 °F | ASTM D5950/D97 |
ExxonMobil SpectraSyn™ 6 Polyalphaolefin (PAO) Fluid Product Description: SpectraSyn™ Low Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties, low volatility, and improved thermal stability. SpectraSyn™ Low Viscosity (PAO) .. |
|||
Pour Point | -57.2 °C | -71.0 °F | ASTM D5950/D97 |
ExxonMobil Exterex™ A41 Synthetic Fluid Product Description: Esterex™ Adipate Esters are API category Group V fluids. These esters have excellent low-temperature properties, high viscosity indices, good lubricating properties and low vol.. |