ExxonMobil SpectraSyn™ 5 Polyalphaolefin (PAO) Fluid

Category Fluid , Lubricant , Polyalphaolefin (PAO)
Manufacturer Exxon Chemical
Trade Name SpectraSyn™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil SpectraSyn™ 5 Polyalphaolefin (PAO) Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: SpectraSyn™ Low Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties, low volatility, and improved thermal stability. SpectraSyn™ Low Viscosity (PAO) products have high viscosity indices which translate to improved flow at low temperatures and increased film thickness at high temperatures. SpectraSyn™ Low Viscosity PAO products are the primary basestocks for synthetic lubricants used in passenger car engines, heavy-duty diesel engines, transmissions, gear boxes and a variety of industrial applications. Appearance: Bright & ClearAvailability: Africa & Middle East, Asia Pacific, Central America, Europe, North America and South AmericaInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.824 g/cc

@Temperature 15.6 °C
0.0298 lb/in³

@Temperature 60.1 °F
ASTM D4052
Viscosity <= 4200 cP

@Temperature -40.0 °C
<= 4200 cP

@Temperature -40.0 °F
Apparent Viscosity by Mini-Rotary Viscometer; ASTM D4684
Viscosity Measurement 138
138
Index; ASTM D2270
Kinematic Viscosity 4920 cSt

@Temperature -40.0 °C
4920 cSt

@Temperature -40.0 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 25 cSt
25 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 5.1 cSt
5.1 cSt
ASTM D445
Thermal Properties Metric English Comments
Pour Point -57.2 °C
-71.0 °F
ASTM D5950/D97
Flash Point 240 °C
464 °F
COC; ASTM D92
Chemical Properties Metric English Comments
Acid Value <= 0.050
<= 0.050
[mg KOH/g]; ASTM D974 (mod)
Descriptive Properties Value Comments
Cold Cranking Simulator 2420 cP
-31°F, ASTM D5293
Color <0.5
ASTM D1500
Composition Water
<50 ppm, ASTM D6304 (mod)
Noack Volatility 0.068
ASTM D5800/DIN 51581