Polymer Property : Pour Point = -73.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Pour Point -73.0 °C
-99.4 °F
Base Oil; ASTM D97
Nye Lubricants 741A (NG) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -73.0 °C
-99.4 °F
Base Oil; ASTM D97
Nye Lubricants 741B (NG) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -73.0 °C
-99.4 °F
Base Oil; ASTM D97
Nye Lubricants 741F (NG) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -73.0 °C
-99.4 °F
Base Oil; ASTM D97
Nye Lubricants 741M (NG) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -73.0 °C
-99.4 °F
Base Oil; ASTM D97
Nye Lubricants 781A (NG) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -73.0 °C
-99.4 °F
Base Oil; ASTM D97
Nye Lubricants 781D (NG) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -73.0 °C
-99.4 °F
Base Oil; ASTM D97
Nye Lubricants 781S (NG) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -73.0 °C
-99.4 °F
Base Oil; ASTM D97
Nye Lubricants 802-1 (FG) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -73.0 °C
-99.4 °F
Base Oil; ASTM D97
Nye Lubricants 813-1 (FG) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -73.0 °C
-99.4 °F
Base Oil; ASTM D97
Nye Lubricants 813S-1 (FG) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -73.0 °C
-99.4 °F
ASTM D97
ChevronTexaco TEGRA® Synthetic Barrier Fluid
Features Chevron Tegra Synthetic Barrier Fluid is formulated to perform as a barrier fluid in dual mechanical seals.Manufactured from the highest quality polyalphaolefin base fluids, it provides pro..
Pour Point -73.0 °C
-99.4 °F
3M Fluorinert™ FC-3284 Electronic Liquid
3M™ Fluorinert™ Liquid FC-3284 is a non-conductive, thermally and chemically stable fluid ideal for use in single and two phase heat transfer fluid applications, such as semiconductor package test..