Polymer Property : Pour Point = 39.2 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Pour Point 4.00 °C
39.2 °F
Base Oil; ASTM D97
Nye Lubricants 438 (SO) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point 4.00 °C
39.2 °F
Base Oil; ASTM D97
Nye Lubricants 718B (NG) Rheolube Grease
Information provided by Nye Lubricants.
Pour Point 4.00 °C
39.2 °F
Base Oil; ASTM D97
Nye Lubricants 718S (NG) Rheolube Grease
Information provided by Nye Lubricants.
Pour Point 4.00 °C
39.2 °F
ASTM D97
ChevronTexaco 250 NC Open Gear Lubricant
FeaturesChevron Open Gear Lubricants are black, viscous lubricants formulated with an asphaltic base and diluted with a nonchlorinated solvent for easy application by hand or through automatic lubri..
Pour Point 4.00 °C
39.2 °F
ASTM D97
ChevronTexaco 250 NC-HT Open Gear Lubricant
FeaturesChevron Open Gear Lubricants are black, viscous lubricants formulated with an asphaltic base and diluted with a nonchlorinated solvent for easy application by hand or through automatic lubri..
Pour Point 4.00 °C
39.2 °F
Solvay RHODASURF® ID/5 Surfactant
Identification: ALCOHOLS, C9-11-ISO, C10-RICH, ETHOXYLATEDCAS: 78330 – 20 – 8Solubility: Soluble in water and most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America and..