Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 650 °C | 1200 °F | |
Plastcom SLOVAMID 6 GF 50 LS PA6, 50% glass fibre, light stability FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Glow Wire Test | 650 °C | 1200 °F | STN IEC 60695-2-10 |
Plastcom SLOVAMID 6 T 15 Polyamide 6, 15% Micronized Talc FeaturesDecreased shrinkage against the BT types, increased heat application up to 170°C. Increased tensile modulus - strength of the material. PA matrix reduction. Application for tools, fillin.. |
|||
Glow Wire Test | 650 °C | 1200 °F | |
Plastcom SLOVAMID 6/66 GF 50 PA6/66, 50% glass fibre FeaturesPA 6/66 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-g.. |
|||
Glow Wire Test | 650 °C | 1200 °F | |
Plastcom SLOVAMID 66 GF 15 TS PA66, 15% glass fibre FeaturesChemically reinforced with 15% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Glow Wire Test | 650 °C @Thickness 2.00 mm |
1200 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYabs N30 ABS Information provided by Polykemi AB |
|||
Glow Wire Test | 650 °C @Thickness 2.00 mm |
1200 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYblend 6005 PC/ABS-Blend Information provided by Polykemi AB |
|||
Glow Wire Test | 650 °C @Thickness 2.00 mm |
1200 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYblend 65FS LB PC/ABS-Blend Information provided by Polykemi AB |
|||
Glow Wire Test | 650 °C @Thickness 2.00 mm |
1200 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYblend C65F PC/ABS-blend Information provided by Polykemi AB |
|||
Glow Wire Test | 650 °C @Thickness 2.00 mm |
1200 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB SCANAMID 66 A12^ QF2515 Nylon 66,Mineral and Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Glow Wire Test | 650 - 960 °C | 1200 - 1760 °F | Average value: 783 °C Grade Count:6 |
Overview of materials for Polystyrene, Heat Resistant Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values.. |
|||
Glow Wire Test | 650 - 700 °C | 1200 - 1290 °F | Average value: 662 °C Grade Count:30 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Glow Wire Test | 650 °C @Diameter 2.00 mm |
1200 °F @Diameter 0.0787 in |
GWIT; IEC 60695-2-13 |
Lanxess Durethan® BKV 115 H3.0 000000 Nylon 6-Copolymer, Glass Fiber Reinforced PA 6-Copolymer, 15% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Glow Wire Test | 650 °C @Diameter 2.00 mm |
1200 °F @Diameter 0.0787 in |
IEC 60695-2-12 |
Lanxess Durethan® BKV 50 H3.0 000000 Nylon 6, 50% Glass Fibers PA 6, 50% glass fibers, injection molding, heat-ageing stabilized |
|||
Glow Wire Test | 650 °C | 1200 °F | IEC 695-2-1 |
Lucite International Diakon® CLG960 Acrylic Polymer Information provided by Lucite International |
|||
Glow Wire Test | 650 °C @Thickness 3.00 mm |
1200 °F @Thickness 0.118 in |
IEC 60695-2-12 |
SABIC Innovative Plastics NORYL WCD801A PPE-TPE Flexible, migration-improved, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements.. |
|||
Glow Wire Test | 650 °C @Thickness 1.60 mm |
1200 °F @Thickness 0.0630 in |
ISO 60695-2-12 |
Solvay TECHNYL® B 218 Black 21 N PA66/6, DRY Description: Unreinforced copolyamide PA 66/6 , heat stabilized , medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL® B 218 offers all of the primary proper.. |
|||
Glow Wire Test | 650 °C @Thickness 1.60 mm |
1200 °F @Thickness 0.0630 in |
ISO 60695-2-12 |
Solvay TECHNYL® C 216 V30 PA6, 30% glass fiber, DRY Description: Polyamide PA6, reinforced with 30 % of glass fiber, for injection molding.Available in: Asia Pacific and Latin AmericaProduct Applications: It has good mechanical properties, it is used.. |
|||
Glow Wire Test | 650 °C @Thickness 1.60 mm |
1200 °F @Thickness 0.0630 in |
ISO 60695-2-12 |
Solvay TECHNYL® C 216 V40 PA6, 40% glass fiber, DRY Description: TECHNYL® C 216 V40 is a polyamide 6, reinforced with 40% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers a good combinati.. |
|||
Glow Wire Test | 650 °C | 1200 °F | IE/CEN 60695-2-12 |
Sax Polymers SAXLAC 310T Acrylonitrile Butadiene Styrene Saxalac 310T is an antistatic, high impact resistant ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provid.. |
|||
Glow Wire Test | 650 °C @Thickness 3.00 mm |
1200 °F @Thickness 0.118 in |
IEC 60695-2-12 |
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus .. |
|||
Glow Wire Test | 650 °C | 1200 °F | GWFI; IEC 60695 |
Polyram RamSter PF306G6 PBT, 30% Glass Fiber 30% Glass fiber reinforced, low viscosity PBT for injection molding applications.Information provided by Polyram. |
|||
Glow Wire Test | 650 °C @Thickness 2.00 mm |
1200 °F @Thickness 0.0787 in |
I.E.C. 695-2-1 |
Cossa Polimeri ESTADIENE 1515 HT Acrylonitrile Butadiene Styrene ABS with high thermal resistanceGood melt flow rate, good impact resistance, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Glow Wire Test | 650 °C @Thickness 2.00 mm |
1200 °F @Thickness 0.0787 in |
I.E.C. 695-2-1 |
Cossa Polimeri ESTADIENE 3015 MT Acrylonitrile Butadiene Styrene ABSMedium thermal resistance, high impact resistance at low temperature, good melt flow rate, high gloss, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Glow Wire Test | 650 °C @Thickness 2.00 mm |
1200 °F @Thickness 0.0787 in |
IEC 60695-2-12 |
Eurostar Staramide AG10K PA66, 50% Glass Filled, Injection Molded AG10 is a Heat and Hydrolytically Stabilized, 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl.. |
|||
Glow Wire Test | 650 °C @Thickness 2.00 mm |
1200 °F @Thickness 0.0787 in |
plaque; IEC 60695 |
Eurotec® Tecomid® NA40 GR30 NL RT PA 6.6 30% glass fiber reinforced, very low friction and wear Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Glow Wire Test | 650 °C @Thickness 2.00 mm |
1200 °F @Thickness 0.0787 in |
plaque; IEC 60695 |
Eurotec® Tecodur® PB70 GR30 NL PBT 30% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Glow Wire Test | 650 °C @Thickness 2.00 mm |
1200 °F @Thickness 0.0787 in |
PN-EN-60695-2-12 |
Azoty Tarnow™ Tarnamid® T-27 MT30 Polyamide 6 - Mineral Reinforced 30% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechani.. |
|||
Glow Wire Test | 650 °C @Thickness 2.00 mm |
1200 °F @Thickness 0.0787 in |
PN-EN-60695-2-12 |
Azoty Tarnow™ Tarnamid® T-27 MW30 Polyamide 6 - Mineral Reinforced 30% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechani.. |
|||
Glow Wire Test | 650 °C @Thickness 1.60 mm |
1200 °F @Thickness 0.0630 in |
ICE 60695-12 |
Akro-Plastic Akromid® B3 GF 40 (2474) PA 6 Dry, 40% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Glow Wire Test | 650 °C | 1200 °F | STN IEC 60695-2-10 |
Plastcom SLOVAMID 6 T 30 Polyamide 6, 30% Micronized Talc FeaturesDecreased shrinkage against the BT types, increased heat application up to 170°C. Increased tensile modulus - strength of the material. PA matrix reduction. Application for tools, fillin.. |