Material Notes:
Flexible, migration-improved, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements. 80C end use temperature rating and good heat deformation performance as defined by UL 1581. 80 Shore A hardness. Processing typically conducted on standard extrusion equipment. UL 1581 tests conducted on 2.0 mm wire with 0.12 mm x 20 stranded copper conductor.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Melt Flow 11 g/10 min

@Load 5.00 kg,
Temperature 250 °C
11 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
30S reading; ASTM D2240
Tensile Strength at Break 12.0 MPa
1740 psi
Type I, 50 mm/min; ASTM D638
13.0 MPa
1890 psi
50 mm/min; ISO 527
16.0 MPa
2320 psi
UL 1581
17.0 MPa
2470 psi
after 7days @113°C; UL 1581
Elongation at Break 119 %
119 %
50 mm/min; ISO 527
120 %
120 %
Type I, 5 mm/min; ASTM D638
145 %
145 %
after 7days @113°C; UL 1581
205 %
205 %
UL 1581
Flexural Modulus 0.0800 GPa
11.6 ksi
12.5 mm/min, 100 mm span; ASTM D790
0.0900 GPa
13.1 ksi
12.5 mm/min; ISO 178
Heat Distortion 16 %

@Load 0.250 kg,
Temperature 100 °C
16 %

@Load 0.551 lb,
Temperature 212 °F
UL 1581
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 80.0 °C
176 °F
UL temperature rating; UL 1581
Brittleness Temperature <= -40.0 °C
<= -40.0 °F
ASTM D746
Flammability, UL94 V-0

@Thickness 4.00 mm
V-0

@Thickness 0.157 in
UL 94
Oxygen Index 26 %
26 %
ISO 4589
Glow Wire Test 750 °C
1380 °F
IEC 60695-2-13
650 °C

@Thickness 3.00 mm
1200 °F

@Thickness 0.118 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 3.80e+15 ohm-cm
3.80e+15 ohm-cm
IEC 60093
Dielectric Constant 2.8

@Frequency 1.00e+6 Hz
2.8

@Frequency 1.00e+6 Hz
IEC 60250
2.8

@Frequency 50.0 - 60.0 Hz
2.8

@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 23.0 kV/mm

@Thickness 2.00 mm
584 kV/in

@Thickness 0.0787 in
in oil; IEC 60243-1
Dissipation Factor 0.0040

@Frequency 1.00e+6 Hz
0.0040

@Frequency 1.00e+6 Hz
IEC 60250
0.030

@Frequency 50.0 - 60.0 Hz
0.030

@Frequency 50.0 - 60.0 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
Smoke Density on 0.5mm plaque, Flame, Ds, max 142
ASTM E 662
Smoke Density on 0.5mm plaque, Non-flame, Ds, max 95
ASTM E 662
VW-1 Pass
UL 1581