Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 110 °C @Thickness 1.50 mm |
230 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PPX-EN-FR3 Modified-PPO, V-1 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
UL RTI, Electrical | 110 °C @Thickness 3.00 mm |
230 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PPX-EN-FR3 Modified-PPO, V-1 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
UL RTI, Electrical | 110 °C @Thickness 1.50 mm |
230 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PPX-FR1 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
UL RTI, Electrical | 110 °C @Thickness 3.00 mm |
230 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PPX-FR1 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
UL RTI, Electrical | 110 °C @Thickness 1.70 mm |
230 °F @Thickness 0.0669 in |
UL 746 |
Polymer Resources PPX-FR1-[color]-EN Modified-PPO, V-0 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
UL RTI, Electrical | 110 °C @Thickness 3.00 mm |
230 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PPX-FR1-[color]-EN Modified-PPO, V-0 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
UL RTI, Electrical | 110 °C @Thickness 3.00 mm |
230 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PPX-FR3 Modified-PPO, V-1 Flame Retardant Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
UL RTI, Electrical | 110 °C @Thickness 3.00 mm |
230 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Delrin® 100P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 100P is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin® 100P provides maximum toughness in the product line without modification. Delrin® 100P has improved pro.. |
|||
UL RTI, Electrical | 110 °C @Thickness 1.50 mm |
230 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Delrin® 100P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 100P is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin® 100P provides maximum toughness in the product line without modification. Delrin® 100P has improved pro.. |
|||
UL RTI, Electrical | 110 °C @Thickness 1.50 mm |
230 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Delrin® 311DP BK402 Acetal Homopolymer
(Unverified Data**) Delrin® 311DP BK402 is a medium high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Informatio.. |
|||
UL RTI, Electrical | 110 °C @Thickness 3.00 mm |
230 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Delrin® 500P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin® 500P has improved processing thermal stability compared to Delrin® 500.Infor.. |
|||
UL RTI, Electrical | 110 °C @Thickness 1.50 mm |
230 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Delrin® 500P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin® 500P has improved processing thermal stability compared to Delrin® 500.Infor.. |
|||
UL RTI, Electrical | 110 °C @Thickness >=1.50 mm |
230 °F @Thickness >=0.0591 in |
|
LG Chemical LUCEL N109LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
UL RTI, Electrical | 110 °C @Thickness >=3.00 mm |
230 °F @Thickness >=0.118 in |
|
LG Chemical LUCEL N109LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
UL RTI, Electrical | 110 °C @Thickness >=1.50 mm |
230 °F @Thickness >=0.0591 in |
|
LG Chemical LUCEL N127LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
UL RTI, Electrical | 110 °C @Thickness >=3.00 mm |
230 °F @Thickness >=0.118 in |
|
LG Chemical LUCEL N127LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
UL RTI, Electrical | 110 °C @Thickness >=0.710 mm |
230 °F @Thickness >=0.0280 in |
|
LG Chemical LUCEL N145LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Electric/Electronic Gears, Automobile speaker HousingCAS No. 66455-31-0Information provided by LG Chemical |
|||
UL RTI, Electrical | 110 °C @Thickness >=1.50 mm |
230 °F @Thickness >=0.0591 in |
|
LG Chemical LUCEL N145LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Electric/Electronic Gears, Automobile speaker HousingCAS No. 66455-31-0Information provided by LG Chemical |
|||
UL RTI, Electrical | 110 °C @Thickness >=3.00 mm |
230 °F @Thickness >=0.118 in |
|
LG Chemical LUCEL N145LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Electric/Electronic Gears, Automobile speaker HousingCAS No. 66455-31-0Information provided by LG Chemical |
|||
UL RTI, Electrical | 110 °C @Thickness >=0.750 mm |
230 °F @Thickness >=0.0295 in |
|
LG Chemical Lupox® TE5006F PET+PC Description: Injection Molding, PET+PC, Flame Retardant, GWIT, CTIApplication: IT/OA, E&E (Connector)CAS No. 68928-70-1, 103598-77-2, 25038-59-9 and 1309-64-4Information provided by LG Chemical |
|||
UL RTI, Electrical | 110 °C @Thickness >=1.50 mm |
230 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOY SR3108FM PC, Halogen Free Flame Retardance Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov.. |
|||
UL RTI, Electrical | 110 °C @Thickness >=3.00 mm |
230 °F @Thickness >=0.118 in |
|
LG Chemical LUPOY SR3108FM PC, Halogen Free Flame Retardance Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov.. |
|||
UL RTI, Electrical | 110 °C @Thickness 3.00 mm |
230 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® MX 1000 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Electrical | 110 °C @Thickness 1.50 mm |
230 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® MX 1002 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Electrical | 110 °C @Thickness 0.750 mm |
230 °F @Thickness 0.0295 in |
|
Eurostar Starflam AFR450X1 PA66, 25% Glass Filled, Injection Molded AFR450X1 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
UL RTI, Electrical | 110 °C @Thickness 0.750 mm |
230 °F @Thickness 0.0295 in |
|
Eurostar Starflam AFR450X2 PA66, 25% Glass Filled, Injection Molded AFR450X2 is a Red Phosphorous, Flame Retardant, 25% Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive su.. |
|||
UL RTI, Electrical | 110 °C @Thickness 3.00 mm |
230 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Delrin® 311DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It has improved dimensional stability, high strengt.. |
|||
UL RTI, Electrical | 110 °C @Thickness 1.50 mm |
230 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Delrin® 588P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 588P NC010 is a medium viscosity acetal homopolymer resin for injection molding. It has good thermal stability, and modifications for more precise molding (reduced warpage, good dimensiona.. |
|||
UL RTI, Electrical | 110 °C @Thickness 3.00 mm |
230 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Delrin® 588P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 588P NC010 is a medium viscosity acetal homopolymer resin for injection molding. It has good thermal stability, and modifications for more precise molding (reduced warpage, good dimensiona.. |
|||
UL RTI, Electrical | 110 °C @Thickness 3.00 mm |
230 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Delrin® 900P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 900P BK602 is a low viscosity black acetal homopolymer resin for multicavity and thin wall molding. It offers an improved processing thermal stability.Information provided by DuPont Perform.. |