Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 140 °C @Thickness 3.00 mm |
284 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Crastin® CE15330 NC010 PBT
(Unverified Data**) Crastin® CE15330 NC010 is a 30% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance.. |
|||
UL RTI, Electrical | 140 °C @Thickness 0.750 mm |
284 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Crastin® LW9030FR BK851 PBT
(Unverified Data**) Crastin® LW9030FR BK851 is a 30% glass fiber reinforced, flame retardant, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional sta.. |
|||
UL RTI, Electrical | 140 °C @Thickness 3.00 mm |
284 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Crastin® LW9030FR BK851 PBT
(Unverified Data**) Crastin® LW9030FR BK851 is a 30% glass fiber reinforced, flame retardant, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional sta.. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 103HSL BKB080 Nylon 66
(Unverified Data**) Zytel® 103HSL BKB080 is a heat stabilized, lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Electrical | 140 °C @Thickness 3.00 mm |
284 °F @Thickness 0.118 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 103HSL BKB080 Nylon 66
(Unverified Data**) Zytel® 103HSL BKB080 is a heat stabilized, lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Electrical | 140 °C @Thickness 3.00 mm |
284 °F @Thickness 0.118 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 45HSB NC010 Nylon 66
(Unverified Data**) Zytel® 45HSB NC010 is a high viscosity, heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
UL RTI, Electrical | 140 °C @Thickness >=0.710 mm |
284 °F @Thickness >=0.0280 in |
|
LG Chemical Lupox® DP1000DU PBT Description: Injection Molding, PBT, General PurposeCAS No. 30965-26-5Information provided by LG Chemical |
|||
UL RTI, Electrical | 140 °C @Thickness >=3.30 mm |
284 °F @Thickness >=0.130 in |
|
LG Chemical Lupox® GP1000S PBT Description: Injection Molding, PBT, General PurposeApplication: Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical |
|||
UL RTI, Electrical | 140 °C @Thickness 0.750 mm |
284 °F @Thickness 0.0295 in |
UL746B |
DSM Arnite® TV4 240 PBT-20% Glass Reinforced (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
UL RTI, Electrical | 140 °C @Thickness 0.710 mm |
284 °F @Thickness 0.0280 in |
UL746B |
DSM Arnite® TV4 261 PBT-30% Glass Reinforced (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL746B |
DSM Stanyl® 46HF5041LW Nylon 46-40% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie.. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL746B |
DSM Stanyl® 46HF5041LW Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
UL RTI, Electrical | 140 °C @Thickness 0.750 mm |
284 °F @Thickness 0.0295 in |
UL746B |
DSM Stanyl® 46HF5041LW Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
UL RTI, Electrical | 140 °C @Thickness 0.710 mm |
284 °F @Thickness 0.0280 in |
UL746B |
DSM Akulon® K224-HG4 Nylon 6-20% Glass Reinforced (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.60 mm |
284 °F @Thickness 0.0630 in |
|
Eurostar Starflam PF0057E PA6, 25% Glass Filled, Injection Molded Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF-1005 Z270)Information provided by Polymer Technology & Services,.. |
|||
UL RTI, Electrical | 140 °C @Thickness 0.750 mm |
284 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R530H BK08 Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H BK08 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R530H Black Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H Black is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. It is specifically designed to maximize the retention of physical properties wh.. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R543H Black Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Black is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, .. |
|||
UL RTI, Electrical | 140 °C @Thickness 0.750 mm |
284 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R543H NT Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H NT is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
UL RTI, Electrical | 140 °C @Thickness 0.710 mm |
284 °F @Thickness 0.0280 in |
UL 746B |
Ascend Performance Materials Vydyne® 66J Nylon 66, General Purpose, high viscosity, DAM Vydyne® 66J is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66J resin offers high strength, .. |
|||
UL RTI, Electrical | 140 °C @Thickness 3.00 mm |
284 °F @Thickness 0.118 in |
UL 746B |
Ascend Performance Materials Vydyne® 66J Nylon 66, General Purpose, high viscosity, DAM Vydyne® 66J is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66J resin offers high strength, .. |
|||
UL RTI, Electrical | 140 °C @Thickness 3.00 mm |
284 °F @Thickness 0.118 in |
UL746B |
DSM Akulon® K223-HMS6 Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Electrical | 140 °C @Thickness 0.750 mm |
284 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R530H NAT Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H NAT is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of ph.. |
|||
UL RTI, Electrical | 140 °C @Thickness 3.00 mm |
284 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R530H NAT Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H NAT is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of ph.. |
|||
UL RTI, Electrical | 140 °C @Thickness 3.00 mm |
284 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R533H NAT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H NAT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |
|||
UL RTI, Electrical | 140 °C @Thickness 0.750 mm |
284 °F @Thickness 0.0295 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® HTN FR52G30BL BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G30BL BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont P.. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL746B |
DSM Arnite® TV4 260 SF PBT-30% Glass Reinforced (European and Asian Grade)
(discontinued **) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
UL RTI, Electrical | 140 °C @Thickness 0.750 mm |
284 °F @Thickness 0.0295 in |
UL746B |
DSM Arnite® TV4 260 SF PBT-30% Glass Reinforced (European and Asian Grade)
(discontinued **) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
UL RTI, Electrical | 140 °C @Thickness 3.00 mm |
284 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Rynite® 545 BK504 PET
(Unverified Data**) Rynite® 545 BK504 is a 45% glass reinforced modified polyethylene terephthalate with good strength and stiffness, excellent dimensional stability and creep resistance.Information provided by DuPont.. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R525H Nat Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H Nat is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |