Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 105 °C @Thickness 1.50 mm |
221 °F @Thickness 0.0591 in |
UL 746 |
PolyOne Maxxam™ FR PP FR 7A11 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 3.00 mm |
221 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PEI-G10 Polyetherimide, 10% Glass Reinforced Polyetherimide, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 3.00 mm |
221 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PEI-G30 Polyetherimide, 30% Glass Reinforced Polyetherimide, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 3.00 mm |
221 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PEI-G40 Polyetherimide, 40% Glass Reinforced Polyetherimide, 40% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness >=1.60 mm |
221 °F @Thickness >=0.0630 in |
|
LG Chemical Lupoy 1302-05 Polycarbonate Resin Description: LUPOY 1302-5 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness >=2.50 mm |
221 °F @Thickness >=0.0984 in |
|
LG Chemical Lupoy 1302-05 Polycarbonate Resin Description: LUPOY 1302-5 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness >=2.50 mm |
221 °F @Thickness >=0.0984 in |
|
LG Chemical Lupoy 1302-07 Polycarbonate Resin Description: LUPOY PC 1302-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness >=1.50 mm |
221 °F @Thickness >=0.0591 in |
|
LG Chemical Lupoy 1303EP-22 Polycarbonate Resin Description: LUPOY PC 1303EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 3.00 mm |
221 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® MX 1000 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness >=1.60 mm |
221 °F @Thickness >=0.0630 in |
|
LG Chemical Lupoy 1302-10 Polycarbonate Resin Description: LUPOY PC 1302-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness >=2.50 mm |
221 °F @Thickness >=0.0984 in |
|
LG Chemical Lupoy 1302-10 Polycarbonate Resin Description: LUPOY PC 1302-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness >=1.60 mm |
221 °F @Thickness >=0.0630 in |
|
LG Chemical Lupoy 1302HP-10 Polycarbonate Resin Description: LUPOY PC 1302HP-10 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness >=2.50 mm |
221 °F @Thickness >=0.0984 in |
|
LG Chemical Lupoy 1302HP-10 Polycarbonate Resin Description: LUPOY PC 1302HP-10 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness >=1.60 mm |
221 °F @Thickness >=0.0630 in |
|
LG Chemical Lupoy 1302UV-08 Polycarbonate Resin Description: LUPOY PC 1302UV-08 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness >=1.50 mm |
221 °F @Thickness >=0.0591 in |
|
LG Chemical Lupoy 1303EP-30 Polycarbonate Resin Description: LUPOY PC 1303EP-30 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 0.800 mm |
221 °F @Thickness 0.0315 in |
|
Solvay TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, DRY Description: TECHNYL® A 60G1 V25 is a 25% GF reinforced organophosphorous flame retarded grade based on a patented high flow polyamide 66 resin. This product is heat stabilized and provides optim.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 0.750 mm |
221 °F @Thickness 0.0295 in |
|
Solvay TECHNYLSTARâ„¢ S 60G1 V30 PA6, 30% glass filled, DRY Description: TECHNYLSTARâ„¢ S 60G1 V30 is a reinforced 30% GF organophosphorous flame retarded grade based on a patented high flow polyamide 6 resin (TechnylStar). This product is heat stabilized.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 3.00 mm |
221 °F @Thickness 0.118 in |
UL 746 |
Teknor Apex Chemlon® 182 Nylon 66, Non-Halogenated Notes: General Purpose; U.L. 94 V-O at 0.57 mm; Colorable; Flame Retardant Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 0.810 mm |
221 °F @Thickness 0.0319 in |
UL 746 |
Teknor Apex Chemlon® 233 GH Nylon, 6, 30% Short Glass Fiber Reinforced Features: Good Dimensional Stability; Good Impact Resistance; Good Processability; Good Toughness; Heat Stabilized; High Strength; Lubricated Processing Method: Injection Molding Forms: Pellets Addi.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 3.00 mm |
221 °F @Thickness 0.118 in |
UL 746 |
Teknor Apex Chemlon® 233 GH Nylon, 6, 30% Short Glass Fiber Reinforced Features: Good Dimensional Stability; Good Impact Resistance; Good Processability; Good Toughness; Heat Stabilized; High Strength; Lubricated Processing Method: Injection Molding Forms: Pellets Addi.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 1.50 mm |
221 °F @Thickness 0.0590 in |
UL 746 |
Teknor Apex Chemlon® 282 Nylon 6, Non-halogenated Features: Flame Retardant; General Purpose; Halogen-free; U.L. 94 V-O at 0.63 mm; ColorableProcessing Method: Injection Molding Forms: Pellets Additive: Flame RetardantInformation Provided by Teknor.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 3.00 mm |
221 °F @Thickness 0.118 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® ST811HS NC010 Nylon 6
(Unverified Data**) Zytel® ST811HS is a flexible, heat stabilized Super Tough polyamide 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores and fastene.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 0.860 mm |
221 °F @Thickness 0.0339 in |
|
Eurostar Starflam RF0023E PA66/6, 10% Glass Filled, Injection Molded Starflam RF0023E is a Mineral Flame Retardant, Halogen Free and Phosphorous Free, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding (also known as RF1002Z230EM)Information provided by Polymer.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 3.00 mm |
221 °F @Thickness 0.118 in |
|
Eurostar Starflam RF0057P PA66/6, 25% Glass Filled, Injection Molded Starflam RF0057P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z270EM)Information provided by Polym.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 0.800 mm |
221 °F @Thickness 0.0315 in |
|
Eurostar Starflam PF0057E PA6, 25% Glass Filled, Injection Molded Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF-1005 Z270)Information provided by Polymer Technology & Services,.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 3.00 mm |
221 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 3.00 mm |
221 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R533 NT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533 NT is general-purpose, 33% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade that is lubricated for good machine feed, flow and mold release. Gl.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 3.00 mm |
221 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R540 Nylon 66, 40% Glass Reinforced, DAM Vydyne® R540 is general-purpose, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 3.00 mm |
221 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R530 NAT Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530 NAT is general-purpose, injection-molding grade, 30% glass-fiber reinforced PA66 resin. Available in natural, it is lubricated for good machine feed, flow and mold releaseAvailability:.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 3.00 mm |
221 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R533 Nylon 66, 33% Glass Filled, Dry as Molded Vydyne® R533 is general-purpose, 33% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for good machine feed, flow, and mold release. Glas.. |