Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 3.00 mm |
167 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC/TP-GP2 PC/Polyester Alloy High Impact, Excellent Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources TP-IGFR-G30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced Warpage Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmen.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 0.710 mm |
167 °F @Thickness 0.0280 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 101F BKB009 Nylon 66
(Unverified Data**) Zytel® 101F BKB009 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness >=2.00 mm |
167 °F @Thickness >=0.0787 in |
|
LG Chemical AF312 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness >=1.50 mm |
167 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical AF312A ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0591 in |
DAM |
Aardvark Polymers Aarlon® 4055FR PA 6/6 Rotational Molding Resin Aarlon 4055FR is a premium flame retardant type 6/6 nylon.Aarlon 4055FR is halogen, heavy metal, and red phosphorus free.Aarlon 4055FR is UL94 V-0 rated.Aarlon 4055FR is semi-crystalline, nucleated,.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 3.00 mm |
167 °F @Thickness 0.118 in |
DAM |
Aardvark Polymers Aarlon® 4055FR PA 6/6 Rotational Molding Resin Aarlon 4055FR is a premium flame retardant type 6/6 nylon.Aarlon 4055FR is halogen, heavy metal, and red phosphorus free.Aarlon 4055FR is UL94 V-0 rated.Aarlon 4055FR is semi-crystalline, nucleated,.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness >=0.550 mm |
167 °F @Thickness >=0.0217 in |
|
LG Chemical Lupox® GP1006FD PBT Description: Injection Molding, PBT, Flame Retardant, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 68928-70-1, 155123-66-3, 24968-12-5 and 1309-64-4Information provided by LG Chemica.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness >=0.800 mm |
167 °F @Thickness >=0.0315 in |
|
LG Chemical Lupox® NH2306F PBT+GF30% Description: Injection Molding, PBT+GF30%, Halogen Free Flame RetardantApplication: IT/OA, E&E (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness >=0.500 mm |
167 °F @Thickness >=0.0197 in |
|
LG Chemical Lupox® TE5006F PET+PC Description: Injection Molding, PET+PC, Flame Retardant, GWIT, CTIApplication: IT/OA, E&E (Connector)CAS No. 68928-70-1, 103598-77-2, 25038-59-9 and 1309-64-4Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0590 in |
UL 746 |
Teknor Apex Chemlon® 223 Nylon 6, Unreinforced Features: Nucleated for fast cyclingProcessing Method: Injection MoldingForms: Pellets Additive: Nucleating AgentInformation Provided by Teknor Apex |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 0.750 mm |
167 °F @Thickness 0.0295 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® FR7025V0F NC010 Nylon 66
(Unverified Data**) Zytel® FR7025V0F NC010 is a flame retardant polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuPont Performance.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 3.00 mm |
167 °F @Thickness 0.118 in |
|
Eurostar Starflam R10002E PA66/6, Injection Molded Starflam R10002E is a Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 66/Polyamide 6 Injection Molding Resin (also known as R1000Z220EM)Information provided by Polymer Te.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 0.710 mm |
167 °F @Thickness 0.0280 in |
UL 746 |
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 43% Filler by Weight Additive:Nucleating AgentLubricant Features:Fast Molding CycleGeneral PurposeGood Mold Release Good.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 0.710 mm |
167 °F @Thickness 0.0280 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPC1 Nylon 66, DAM Vydyne® 21SPC1 is a general-purpose, improved-flow, lubricated PA66 resin available in natural color. 21SPC1 offers a balanced combination of properties characterized by high strength, rigidity, go.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 3.00 mm |
167 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, Conditioned Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 3.00 mm |
167 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPF Nylon 66, General Purpose, High Productivity, DAM Vydyne® 21SPF is general-purpose PA66 resin. Available in natural, it is designed principally for injection-molding fabrication. This grade offers a well-balanced combination of engineering propert.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 0.710 mm |
167 °F @Thickness 0.0280 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPG1 Nylon 66, DAM Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPG1 Nylon 66, DAM Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 0.750 mm |
167 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® 41H BK03 Nylon 66, Impact Modified, DAM Vydyne® 41H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, DAM Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H BK0644 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0644 is a high-performance, medium-impact-modified, heat-stabilized PA66 resin with excellent UV stability and outstanding processing characteristics. This product has an UL746C f1 ra.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 3.00 mm |
167 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 49 Nylon 66, Impact Modified, DAM Vydyne® 49 is general-purpose, impact-modified PA66 resin. Available in natural, is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact s.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 3.00 mm |
167 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 64C-R Nylon 66, DAM Vydyne® 64C-R is a medium-viscosity PA66 resin suitable for injection-molding, extrusion and compounding applications. It is available in natural color only. Vydyne 64C-R resin offers high strength.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 3.00 mm |
167 °F @Thickness 0.118 in |
UL 746B |
Ascend Performance Materials Vydyne® 66B Nylon 66, General Purpose, high viscosity, DAM Vydyne® 66B is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66B resin offers high strength, .. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 0.750 mm |
167 °F @Thickness 0.0295 in |
UL746B |
DSM Arnite® A04 900 PET (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 3.00 mm |
167 °F @Thickness 0.118 in |
UL 746B |
Ascend Performance Materials Vydyne® 50BWFS Nylon 66, Dry as Molded Vydyne® 50BWFS is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a highviscosity resin. This resin offers a well-balanced com.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 0.400 mm |
167 °F @Thickness 0.0157 in |
UL 746 |
Ascend Performance Materials Vydyne® ECO366 Nylon 66, Flame-retardant, DAM Vydyne® ECO366 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for machin.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 0.710 mm |
167 °F @Thickness 0.0280 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® EFE1068 NC010T Nylon 66
(Unverified Data**) Zytel® EFE1068 NC010T is a lubricated polyamide 66 for injection molding. It has excellent flow characteristics and was developed for fast production cycles and high productivity applications.Info.. |