Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : UL RTI, Mechanical without Impact = 212 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
UL RTI, Mechanical without Impact 100 °C

@Thickness >=0.710 mm
212 °F

@Thickness >=0.0280 in
LG Chemical LUCEL N109LD POM, Chemical Resistance
Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical
UL RTI, Mechanical without Impact 100 °C

@Thickness >=1.50 mm
212 °F

@Thickness >=0.0591 in
LG Chemical LUCEL N109LD POM, Chemical Resistance
Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical
UL RTI, Mechanical without Impact 100 °C

@Thickness >=3.00 mm
212 °F

@Thickness >=0.118 in
LG Chemical LUCEL N109LD POM, Chemical Resistance
Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical
UL RTI, Mechanical without Impact 100 °C

@Thickness >=3.00 mm
212 °F

@Thickness >=0.118 in
LG Chemical LUCEL N127LD POM, Chemical Resistance
Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical
UL RTI, Mechanical without Impact 100 °C

@Thickness >=3.00 mm
212 °F

@Thickness >=0.118 in
LG Chemical LUCEL N145LD POM, Chemical Resistance
Feature: Injection Molding, POM, Chemical ResistanceApplication: Electric/Electronic Gears, Automobile speaker HousingCAS No. 66455-31-0Information provided by LG Chemical
UL RTI, Mechanical without Impact 100 °C

@Thickness >=0.750 mm
212 °F

@Thickness >=0.0295 in
LG Chemical LUMID GP2251BF PA66+GF25%, Flame Retardant
Feature: Injection Molding, PA66+GF25%, Flame RetardantApplication: IT/OA (Micro Switch)CAS No. 32131-17-2, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Chemical
UL RTI, Mechanical without Impact 100 °C

@Thickness >=0.750 mm
212 °F

@Thickness >=0.0295 in
LG Chemical LUMID GP2301BF PA 66+GF30%, Flame Retardant
Feature: Injection Molding, PA 66+GF30%, Flame RetardantApplication: IT/OA (Micro Switch, ConnectorCAS No. 32131-17-2, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Che..
UL RTI, Mechanical without Impact 100 °C

@Thickness 1.50 mm
212 °F

@Thickness 0.0591 in
DAM; UL 746B
DuPont Performance Polymers Zytel® ST811HS NC010 Nylon 6  (Unverified Data**)
Zytel® ST811HS is a flexible, heat stabilized Super Tough polyamide 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores and fastene..
UL RTI, Mechanical without Impact 100 °C

@Thickness 0.750 mm
212 °F

@Thickness 0.0295 in
Eurostar Starflam AFR470X2 PA66, 35% Glass Filled, Injection Molded
AFR470X2 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
UL RTI, Mechanical without Impact 100 °C

@Thickness 0.400 mm
212 °F

@Thickness 0.0157 in
UL 746
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM
Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri..
UL RTI, Mechanical without Impact 100 °C

@Thickness 0.750 mm
212 °F

@Thickness 0.0295 in
UL 746
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM
Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri..
UL RTI, Mechanical without Impact 100 °C

@Thickness 1.50 mm
212 °F

@Thickness 0.0591 in
UL 746
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM
Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri..
UL RTI, Mechanical without Impact 100 °C

@Thickness 0.750 mm
212 °F

@Thickness 0.0295 in
UL 746B
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, DAM
Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla..
UL RTI, Mechanical without Impact 100 °C

@Thickness 0.400 mm
212 °F

@Thickness 0.0157 in
UL 746B
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, DAM
Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla..
UL RTI, Mechanical without Impact 100 °C

@Thickness 1.50 mm
212 °F

@Thickness 0.0591 in
UL 746B
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, DAM
Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla..
Copyright © lookpolymers.com All Rights Reserved