Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, Unreinforced
Manufacturer Ascend Performance Materials (formerly Solutia)
Trade Name VYDYNE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwriters Laboratories UL 94 flammability classification of V-0 at 0.4 mm (0.016”) thick.Availability:Asia PacificEuropeNorth America Additive:Flame RetardantLubricant Features:DuctileFlame RetardantGood Crack ResistanceGood Mold ReleaseGood ToughnessHalogen FreeHigh ElongationLow DensityLubricatedUses:AppliancesAutomotive ElectronicsBobbinsConnectorsElectrical HousingElectrical PartsElectrical/Electronic ApplicationsFastenersIndustrial ApplicationsLighting ApplicationsLiving HingesPrinted Circuit BoardsSwitchesAppearance: BlackForms: PelletsProcessing Method: Injection MoldingInformation provided by Ascend Performance Materials.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ISO 1183
Water Absorption 0.80 %

@Time 86400 sec
0.80 %

@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 2.3 %
2.3 %
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.012 cm/cm

@Diameter 2.00 mm
0.012 in/in

@Diameter 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.014 cm/cm

@Diameter 2.00 mm
0.014 in/in

@Diameter 0.0787 in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 5.50 MPa
798 psi
ISO 527-2
Tensile Strength, Yield 75.0 MPa
10900 psi
ISO 527-2
Tensile Modulus 5.00 GPa
725 ksi
ISO 527-2
Flexural Strength 92.0 MPa
13300 psi
ISO 178
Flexural Modulus 3.20 GPa
464 ksi
ISO 178
Poissons Ratio 0.40
0.40
ISO 527-2
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
ISO 180
Charpy Impact Unnotched NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179/1eU
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.540 J/cm²

@Temperature -30.0 °C
2.57 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
0.540 J/cm²

@Temperature 23.0 °C
2.57 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 11.0 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
6.11 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
CTE, linear, Transverse to Flow 11.0 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
6.11 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
Melting Point 244 °C
471 °F
ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 225 °C
437 °F
Unannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
Unannealed; ISO 75-2/A
UL RTI, Electrical 130 °C

@Thickness 0.400 mm
266 °F

@Thickness 0.0157 in
UL 746
130 °C

@Thickness 0.750 mm
266 °F

@Thickness 0.0295 in
UL 746
130 °C

@Thickness 1.50 mm
266 °F

@Thickness 0.0591 in
UL 746
130 °C

@Thickness 3.00 mm
266 °F

@Thickness 0.118 in
UL 746
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 0.400 mm
149 °F

@Thickness 0.0157 in
UL 746
65.0 °C

@Thickness 0.750 mm
149 °F

@Thickness 0.0295 in
UL 746
85.0 °C

@Thickness 1.50 mm
185 °F

@Thickness 0.0591 in
UL 746
85.0 °C

@Thickness 3.00 mm
185 °F

@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact 100 °C

@Thickness 0.400 mm
212 °F

@Thickness 0.0157 in
UL 746
100 °C

@Thickness 0.750 mm
212 °F

@Thickness 0.0295 in
UL 746
100 °C

@Thickness 1.50 mm
212 °F

@Thickness 0.0591 in
UL 746
110 °C

@Thickness 3.00 mm
230 °F

@Thickness 0.118 in
UL 746
Flammability, UL94 V-0

@Thickness 0.400 mm
V-0

@Thickness 0.0157 in
V-0

@Thickness 0.750 mm
V-0

@Thickness 0.0295 in
V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Oxygen Index 29 %
29 %
ISO 4589-2
Glow Wire Test 725 °C

@Thickness 3.00 mm
1340 °F

@Thickness 0.118 in
Ignition Temperature; IEC 60695-2-13
775 °C

@Thickness 1.50 mm
1430 °F

@Thickness 0.0591 in
Ignition Temperature; IEC 60695-2-13
875 °C

@Thickness 0.400 mm
1610 °F

@Thickness 0.0157 in
Ignition Temperature; IEC 60695-2-13
875 °C

@Thickness 0.750 mm
1610 °F

@Thickness 0.0295 in
Ignition Temperature; IEC 60695-2-13
960 °C

@Thickness 0.400 mm
1760 °F

@Thickness 0.0157 in
Flammability Index; IEC 60695-2-12
960 °C

@Thickness 0.750 mm
1760 °F

@Thickness 0.0295 in
Flammability Index; IEC 60695-2-12
960 °C

@Thickness 1.50 mm
1760 °F

@Thickness 0.0591 in
Flammability Index; IEC 60695-2-12
960 °C

@Thickness 3.00 mm
1760 °F

@Thickness 0.118 in
Flammability Index; IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm

@Thickness 0.750 mm
1.00e+11 ohm-cm

@Thickness 0.0295 in
IEC 60093
Dielectric Strength 13.0 kV/mm

@Thickness 1.00 mm
330 kV/in

@Thickness 0.0394 in
IEC 60243
Arc Resistance 120 - 179 sec

@Thickness 3.00 mm
120 - 179 sec

@Thickness 0.118 in
ASTM D495
Comparative Tracking Index 600 V

@Thickness 3.00 mm
600 V

@Thickness 0.118 in
IEC 60112
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 0.400 mm
7.0 - 14 sec

@Thickness 0.0157 in
UL 746
7.0 - 14 sec

@Thickness 0.750 mm
7.0 - 14 sec

@Thickness 0.0295 in
UL 746
7.0 - 14 sec

@Thickness 1.50 mm
7.0 - 14 sec

@Thickness 0.0591 in
UL 746
15 - 29 sec

@Thickness 3.00 mm
15 - 29 sec

@Thickness 0.118 in
UL 746
High Amp Arc Ignition, HAI >= 120 arcs

@Thickness 0.400 mm
>= 120 arcs

@Thickness 0.0157 in
UL 746
>= 120 arcs

@Thickness 0.750 mm
>= 120 arcs

@Thickness 0.0295 in
UL 746
>= 120 arcs

@Thickness 1.50 mm
>= 120 arcs

@Thickness 0.0591 in
UL 746
>= 120 arcs

@Thickness 3.00 mm
>= 120 arcs

@Thickness 0.118 in
UL 746
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Processing Properties Metric English Comments
Rear Barrel Temperature 240 - 270 °C
464 - 518 °F
Middle Barrel Temperature 240 - 270 °C
464 - 518 °F
Front Barrel Temperature 240 - 270 °C
464 - 518 °F
Nozzle Temperature 240 - 270 °C
464 - 518 °F
Melt Temperature 250 - 270 °C
482 - 518 °F