Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 155 °C @Thickness 0.750 mm |
311 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Rynite® FR530 BK507 PET
(Unverified Data**) Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 155 °C @Thickness 1.50 mm |
311 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Rynite® FR530 BK507 PET
(Unverified Data**) Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 155 °C @Thickness 2.00 mm |
311 °F @Thickness 0.0787 in |
UL 746B |
DuPont Performance Polymers Rynite® FR530 BK507 PET
(Unverified Data**) Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 155 °C @Thickness 3.00 mm |
311 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Rynite® FR530 BK507 PET
(Unverified Data**) Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 155 °C @Thickness 3.00 mm |
311 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Rynite® FR530L BK507 PET
(Unverified Data**) Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 155 °C @Thickness 3.00 mm |
311 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Rynite® FR530L BK507 PET
(Unverified Data**) Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 155 °C @Thickness 2.00 mm |
311 °F @Thickness 0.0787 in |
UL 746B |
DuPont Performance Polymers Rynite® FR530L BK507 PET
(Unverified Data**) Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 155 °C @Thickness 1.50 mm |
311 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Rynite® FR530L BK507 PET
(Unverified Data**) Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 155 °C @Thickness 1.50 mm |
311 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Rynite® FR530L BK507 PET
(Unverified Data**) Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 155 °C @Thickness 0.750 mm |
311 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Rynite® FR530L BK507 PET
(Unverified Data**) Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 155 °C @Thickness 2.00 mm |
311 °F @Thickness 0.0787 in |
UL 746B |
DuPont Performance Polymers Rynite® FR530L BK507 PET
(Unverified Data**) Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |