Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
Polimeri Europa Eraclene® FC 82 High Density Polyethylene - Blown Film Extrusion Eraclene FC 82 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Its broad molecular weight distribution and density successfully co.. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
Polimeri Europa Eraclene® MM 74 U High Density Polyethylene - Injection Molding Eraclene MM 74 U is a gas phase high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.This grade has a narrow molecular weight distribution. The polym.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R881C Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | TPE-0089 (ASTM D 746) |
ExxonMobil Vyram™ 9271-55 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic elastomer which complies with FDA regulations for rubber articles intended for repeated use, as well as rubber articles in contact with non-fatty, non-oily foods as closure.. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
Polimeri Europa Eraclene® MS 80 High Density Polyethylene - Injection Molding Eraclene MS 80 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MS 80 shows a good balance between processability and mechanical pro.. |
|||
Brittleness Temperature | -60.0 - -57.0 °C | -76.0 - -70.6 °F | Average value: -59.0 °C Grade Count:4 |
Overview of materials for Styrenic TPE
(Unverified Data**) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic TPE". Each property range of values reported is minimum and maximum values of appropriate MatWe.. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D696 |
NOVA Chemicals Sclair® 11P3 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent seal characteristics, easy processability.Applications: Specialty lamination, co-extrusion.Data provided by the manufacturer. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D696 |
NOVA Chemicals Sclair® 11P4 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent sealing characteristics, easy processability.Applications: Specialty lamination, co-extrusion.Data provided by the manufacturer. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
Chevron Phillips HiD® 9720 HDPE Injection Molding Resin
(discontinued **) Resin Type: linear homopolymerCharacteristics: good flow, moderate impact strength, excellent stiffness, moderate ESCR, moderate shrinkage resistanceApplications: pails, structural foamInformation p.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | |
Momentive Performance Materials N-Sil® RTV122 Silicone Modified Alkoxy Adhesive Sealants, White N-Sil® adhesive sealants are one-component, ready-to-use, and cure to a tough, resilient silicone rubber on exposure to atmospheric moisture at room temperature.Key Performance Properties: Primer.. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | |
Teknor Apex Elexar® EL 3954-62 Thermoplastic Elastomer Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop.. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
SCG Chemicals EL-Leneâ„¢ H1000PWI High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stability, good resistance to weathering, reduce heat conductivity to waterRecommended Applications: Above ground pipes, double wall pipesInforma.. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
SCG Chemicals EL-Leneâ„¢ H1000PYL High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stability, good resistance to weatheringRecommended Applications: Stripe lines for PE100 pipe, non pressure pipesCertification: Certified by LNE.. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
SCG Chemicals EL-Leneâ„¢ H6430BM High Density Polyethylene Blow Molding Key Characteristics:Excellent stiffnessGood processabilityOdorlessSafe for food contactGood printabilityRecommended Applications:Bottles for drinking water, fruit juice, soft drink, milkAutomotive p.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with TP-759 Plasticizer MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
Teknor Apex TEKRON® 4300LM-P86-1 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
Teknor Apex Telcar® TL-1138 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
Teknor Apex UNIPRENE® 7100-73 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
Teknor Apex Uniprene® UN-2028A UMB Thermoplastic Elastomer Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D 746 |
Zylog Neoplast® 155 FT EB Thermoplastic Vulcanizate Neoplast 155 FT EB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding and Extrusion applications.RoHS Compliant, .. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | |
Arlon CuClad 6250 Bonding Film Thermoplastic Bonding FilmsSimilar Dk and Df range to many PTFE laminatesBenefits:Can be reheated to remelt and reflow bonding filmExcellent Electrical PropertiesTypical Applications:Stripline Circu.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D746 |
Alliance Polymers Viprene™ G45D-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G45D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D746 |
Alliance Polymers Viprene™ G65A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G65A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D746 |
Alliance Polymers Viprene™ G90A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G90A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | |
AlphaGary Garaflex™ G 7782-A4 Thermoplastic Elastomer Garaflex™ G is a thermoplastic elastomer intended for wire and cable applications105°C rated TPE for flexible cord (SEO & SJEO). |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D746 |
Alliance Polymers Viprene™ G85A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G85A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D 746 |
AlphaGary Evoprene™ LF 6151 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
Polimeri Europa Eraclene® FA 506 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion Eraclene FA 506 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Its broad molecular weight distribution and density successfully c.. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
Polimeri Europa Eraclene® MM 84 U High Density Polyethylene - Injection Molding Eraclene MM 84 U is a gas phase high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MM 84 U is characterized by high rigidity and good impac.. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
SCG Chemicals EL-Lene™ H5211PYL High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stability, good resistance to weatheringRecommended Applications: Stripe lines for PE80 pipe, non pressure pipesCertification: Certified by LNEI.. |