Thermal Properties Metric English Comments
Brittleness Temperature -135 °C
-211 °F
ASTM D746
SABIC Innovative Plastics Lexan® FR66 Polycarbonate Film, Flame Retardant
Lexan FR66 flame-retardant film is a clear, thin-gauge polycarbonate film with a suede finish on one side and a matte finish on the other, and a UL94 V-0 listing to meet the stringent requirements i..
Brittleness Temperature -135 °C
-211 °F
ASTM D746
SABIC Innovative Plastics Lexan® FR700 Polycarbonate Film, Flame Retardant
Lexan FR700 is a black, one side fine matt, one side velvet flame-retardant polycarbonate film with a UL94 V-0 listing at 0.250 mm. This film has formability, excellent mechanical properties, good d..
Brittleness Temperature -135 °C
-211 °F
ASTM D746
SABIC Innovative Plastics Lexan® FR83 Polycarbonate Film, Flame Retardant
Lexan* FR83 flame-retardant film is a matt/polished, thin-gauge polycarbonate film with a UL94 VTM-0 listing to meet the stringent requirements in a wide range of electrical, electronic and transpor..
Brittleness Temperature -135 °C
-211 °F
ASTM D746
SABIC Innovative Plastics Lexan® FR60 Polycarbonate Film, Flame Retardant
Lexan FR60 flame-retardant film is a clear, thin-gauge polycarbonate film with polished surfaces on both sides, and a UL94 V-0 listing to meet the stringent requirements in a wide range of electrica..
Brittleness Temperature -135 °C
-211 °F
ASTM D746
SABIC Innovative Plastics Lexan® FR63 Polycarbonate Film, Flame Retardant
Lexan FR63 flame-retardant film is a clear, thin-gauge polycarbonate film with a matte finish on one side and a polish finish on the other and a UL94 V-0 listing to meet the stringent requirements i..
Brittleness Temperature -135 °C
-211 °F
ASTM D746
SABIC Innovative Plastics Lexan® FR735A Polycarbonate Film, Flame Retardant
Lexan FR735A is a black, one side velvet, one polish flame-retardant polycarbonate film with a UL94 V-0 listing at 0.250 mm. This film has formability, excellent mechanical properties, good dimensio..
Brittleness Temperature -135 °C
-211 °F
ASTM D746
SABIC Innovative Plastics Valox® FR1 Polybutylene Terephthalate Film, Flame Retardant
Valox FR-1 film is a flame retardant thermoplastic polybutylene, terephthalite film offering UL94 VTM-0 performance down to 125 microns and good temperature performance. Valox FR-1 film’s outst..
Brittleness Temperature -135 °C
-211 °F
ASTM D746
SABIC Innovative Plastics Lexan® FR65 Polycarbonate Film, Flame Retardant
Lexan FR65 flame-retardant film is a clear, thin-gauge polycarbonate film with a velvet finish on one side and a matt finish on the other, and a UL94 V-0 listing to meet the stringent requirements i..