Teknor Apex APEX® 65002 Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® 65002 Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: 105°C Jacket; RoHS Compliant Features: Flame Retardant; Lead-free Uses: Communication Wire JacketingForms: Pellets Agency Ratings: NEC Article 725; NEC Article 760; NEC Article 770; NEC Article 800; UL 13; UL 1424; UL 444Wire Types: CL2; CL3; CM; FPL; MP; OFN Processing Method: Extrusion Additional Information: Temperature Rating: 105°C UL Sunlight Resistance Recognition: No Formerly 95-A0542E-99Information Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore C 73
73
10 seconds; ASTM D2240
Tensile Strength at Break 22.1 MPa
3200 psi
ASTM D638
Elongation at Break 340 %
340 %
ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -28.0 °C
-18.4 °F
ASTM D746
Oxygen Index 30 %
30 %
ASTM D2863
Processing Properties Metric English Comments
Melt Temperature 191 °C
375 °F
Descriptive Properties Value Comments
Appearance Opaque