Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -34.4 °C | -29.9 °F | ASTM D746 |
PolyOne Geon™ HC 2165 Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2165 is a 65 Shore A non-phthalate flexible vinyl compound made from FDA sanctioned ingredients. HC 2165 can be used for extrusion and injection molding healthcare applications.NOTE: All ing.. |
|||
Brittleness Temperature | -34.4 °C | -29.9 °F | ASTM D746 |
PolyOne Geon™ HC 2165G Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2165G is a 65 Shore A non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 2165G can be used for extrusion and injection molding healthcare applicatio.. |
|||
Brittleness Temperature | -34.4 °C | -29.9 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible A65M0 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Brittleness Temperature | -34.4 °C | -29.9 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible B8501 Polyvinyl Chloride, Flexible (PVC, Flexible) A flexible Vinyl compound for hose and tubing applications with enhanced physical characteristics.Information provided by PolyOne |
|||
Brittleness Temperature | -34.4 °C | -29.9 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible 86273 Trans 002 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -34.4 °C | -30.0 °F | ASTM D746 |
Seals Eastern 7042 Fluorocarbon-Elastomer Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type.. |
|||
Brittleness Temperature | -34.4 °C | -30.0 °F | ASTM D746 |
Teknor Apex APEX® 01-A0087A-91 Polyvinyl Chloride, Flexible Notes: 75°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex |