Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -36.0 °C | -32.8 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable JA306BA Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | <= -36.0 °C | <= -32.8 °F | ASTM D746 |
S&E Specialty Polymers CPE-01-266LT PVC Application: 90°C, oil resistant CPE based, FT4, 210,000 BTU wire and cable jacketing material with enhanced low temperature properties.Information provided by S&E Specialty Polymers |
|||
Brittleness Temperature | -36.0 °C | -32.8 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R7545H Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -36.0 °C | -32.8 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible XV3805 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Brittleness Temperature | -36.0 °C | -32.8 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable MLA71A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -36.0 °C | -32.8 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable W3400L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Brittleness Temperature | <= -36.0 °C | <= -32.8 °F | ASTM D746 |
Eastman 18DOA Polyethylene
(discontinued **) Polyethylene 18DOA is a low density formulation suggested for the production of closures where a high melt index material is needed to meet shrinkage requirements and fast molding cycles. It molds .. |
|||
Brittleness Temperature | -36.0 °C | -32.8 °F | ASTM D746 |
Teknor Apex APEX® 3300-75 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med.. |
|||
Brittleness Temperature | -36.0 °C | -32.8 °F | ASTM D746 |
Teknor Apex APEX® 3601-75 Polyvinyl Chloride, Flexible Uses: Medical/Healthcare Applications Agency Ratings: NSF 61 Forms: Pellets Additional Information: Second Generation SeriesInformation Provided by Teknor Apex |
|||
Brittleness Temperature | -36.0 °C | -32.8 °F | ASTM D746 |
Teknor Apex APEX® 80-C118-R Polyvinyl Chloride, Flexible Notes: 105°C Insulation; RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex |
|||
Brittleness Temperature | -36.0 °C | -32.8 °F | ASTM D746 |
Teknor Apex Flexalloy® 3500-80 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MWUses- Tubing, Pump PartsForms-PelletsProcessing- ExtrusionInformation provided by Te.. |
|||
Brittleness Temperature | -36.0 °C | -32.8 °F | ASTM D746 |
Teknor Apex APEX® 3200-75 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Brittleness Temperature | -36.0 °C | -32.8 °F | ASTM D746 |
Teknor Apex APEX® 3300-80 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med.. |
|||
Brittleness Temperature | -36.0 °C | -32.8 °F | ASTM D746 |
Teknor Apex APEX® 3300R-75NT Polyvinyl Chloride, Flexible Notes: RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex |
|||
Brittleness Temperature | -36.0 °C | -32.8 °F | |
Sylvin Technologies 6119-68 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Brittleness Temperature | -36.0 °C | -32.8 °F | |
A. Schulman POLYTROPE™ TPP 1010HF-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1010HF-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristic.. |
|||
Brittleness Temperature | -36.0 °C | -32.8 °F | |
A. Schulman POLYTROPE™ TPP 1010HF-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1010HF-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristic.. |
|||
Brittleness Temperature | -36.0 °C | -32.8 °F | |
A. Schulman POLYTROPE™ TPP 1010HF-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1010HF-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristic.. |
|||
Brittleness Temperature | -36.0 °C | -32.8 °F | |
A. Schulman POLYTROPE™ TPP 1010HF-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1010HF-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristic.. |
|||
Brittleness Temperature | -36.0 °C | -32.8 °F | |
A. Schulman POLYTROPE™ TPP 1010HF-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1010HF-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristic.. |
|||
Brittleness Temperature | -36.0 °C | -32.8 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds CKL 70 Flexible PVC, Sheathing Lead Free General purposes |
|||
Brittleness Temperature | -36.0 °C | -32.8 °F | Temperature Retraction, TR-10 |
Dow Nordel® IP 4640 Low Cost General Purpose Hose FormulationNordel® IP 4640 |
|||
Brittleness Temperature | -36.0 °C | -32.8 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds FR 70 Flexible PVC, Insulation Good flexibility cables |
|||
Brittleness Temperature | -36.0 °C | -32.8 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PH 60 Flexible PVC, Transparent Extrusion Transparent profiles |
|||
Brittleness Temperature | -36.0 °C | -32.8 °F | ASTM D-746 |
Axiall 17883 Wire & Cable Flexible PVC UV resistant, 90C insulation compound with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -36.0 °C | -32.8 °F | ASTM D-746 |
Axiall 375 Wire & Cable Flexible PVC General purpose and AWM flame retardant jacket. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -36.0 °C | -32.8 °F | ASTM D-746 |
Axiall 38601 Coax & Telecom Flexible PVC CATV and general purpose jacket. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -36.0 °C | -32.8 °F | ASTM D746 |
Teknor Apex APEX® 3201-75 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Brittleness Temperature | -36.0 °C | -32.8 °F | |
Sylvin Technologies 60509 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Brittleness Temperature | -36.0 °C | -32.8 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PMP 338 Flexible PVC, Extrusion Modified with PU Sheath PVC/PU for low temperatures |