Polymer Property : Brittleness Temperature = -43.9 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Brittleness Temperature -43.9 °C
-47.0 °F
ASTM D746
PolyOne Geon™ Vinyl Wire & Cable WJKC505L Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide..
Brittleness Temperature -43.9 °C
-47.0 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible A7501 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne
Brittleness Temperature -43.9 °C
-47.0 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible B7500 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Brittleness Temperature -43.9 °C
-47.0 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible K85 Natural & Black Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Brittleness Temperature -43.9 °C
-47.0 °F
ASTM 746
ExxonMobil Vyram™ 9103-45 Thermoplastic Elastomer  (discontinued **)
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
Brittleness Temperature -43.9 °C
-47.0 °F
ASTM 746
ExxonMobil Vyram™ 9203-45 Thermoplastic Elastomer  (discontinued **)
A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character..
Brittleness Temperature -43.9 °C
-47.0 °F
ASTM D746
PolyOne Geon® XV3811B Thermoplastic Elastomer - PVC/TPU  (discontinued **)
Applications:Hose and TubingCustom ProfilesProcessing Method:Extrusion and MoldingExtrusion-ProfileInformation provided by PolyOne Corporation.
Brittleness Temperature -43.9 °C
-47.0 °F
ASTM D746
ExxonMobil LD 509.48 Compounding Resin  (discontinued **)
LD 509.48 is a high melt index homopolymer resin designed to provide good processability in compounding applications.Information provided by ExxonMobil Chemical
Brittleness Temperature -43.9 °C
-47.0 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible A7500 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne
Brittleness Temperature -43.9 °C
-47.0 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible C6501 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Brittleness Temperature -43.9 °C
-47.0 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible R5165A Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Brittleness Temperature -43.9 °C
-47.0 °F
ASTM D746-79
Saint-Gobain Transflow® M-34-R Raw Milk Tubing Formulation
Description: Transflow M-34-R: Transflow Raw Milk tubing is specially formulated to reduce the risks that can occur with the use of rubber tubings. Many regulatory sanitarians throughout the w..
Brittleness Temperature -43.9 °C
-47.0 °F
ASTM D746-98
Saint-Gobain Vendflow® E-70-V-CE Taste Barrier Tubing Formulation
Description: Non-plasticized inner bore yeilds no taste: Vendflow® E-70-V-CE is specifically formulated to transfer water and beverages without imparting any "plastic" taste sometimes found in PV..
Brittleness Temperature -43.9 °C
-47.0 °F
ASTM D746; ISO 812
Advanced Polymer Alloys Alcryn® 1080 BK Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..