Polymer Property : Brittleness Temperature = -52.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Brittleness Temperature -52.0 °C
-61.6 °F
ASTM D746
PolyOne Synprene™ RT-5180 RoHS Natural Styrene Butadiene Block Copolymer (SBC)
Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom..
Brittleness Temperature -52.0 °C
-61.6 °F
ASTM D746
Eastman 1390P Polyethylene  (discontinued **)
Low-density polyethylene 1390P is used primarily in extrusion-coating applications that require fast line speeds and relatively low coating weights. When compared with other low-density polyethylen..
Brittleness Temperature -52.0 °C
-61.6 °F
ASTM D746
PolyOne Synprene® RT-5180 Styrene Butadiene Block Copolymer (SBC)  (discontinued **)
Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom..
Brittleness Temperature -52.0 °C
-61.6 °F
ASTM D746
Kraton® G7820 GU-N (SEBS) Compound
Description: Kraton G7820 GU-N is an easy processing, general purpose 90 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form..
Brittleness Temperature -52.0 °C
-61.6 °F
ASTM D746
Teknor Apex APEX® 2555-H Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin..
Brittleness Temperature -52.0 °C
-61.6 °F
ASTM D746
Teknor Apex APEX® 4168 Polyvinyl Chloride Compound
Notes: Sunlight Resistant Jacket Temperature Rating: 75°CInformation Provided by Teknor Apex
Brittleness Temperature -52.0 °C
-61.6 °F
ASTM D746
Teknor Apex APEX® 4168 Polyvinyl Chloride, Flexible
Information Provided by Teknor Apex
Brittleness Temperature -52.0 °C
-61.6 °F
ASTM D746
Teknor Apex APEX® 94-A0098C-45 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose Uses-General PurposeAppearance-ClearForms-PelletsProcessing Method-Injection Molding..
Brittleness Temperature -52.0 °C
-61.6 °F
ASTM D746
Teknor Apex Flexalloy® 3500-50 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MWUses- Tubing, Pump PartsForms-PelletsProcessing- ExtrusionInformation provided by Te..
Brittleness Temperature -52.0 °C
-61.6 °F
ASTM D746
Teknor Apex Flexalloy® 3501-50-NT Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MW, Ethylene Oxide SterilizableForms-PelletsProcessing-Extrusion, Injection MoldingAppe..
Brittleness Temperature -52.0 °C
-61.6 °F
ASTM D746
Teknor Apex Flexalloy® 9606-65 Polyvinyl Chloride, Elastomer
Notes: 105°C Jacket; RoHS Compliant Features: Flame Retardant; High Heat Resistance; Low Temperature Flexibility; Sunlight Resistant (720 hours) Uses Cable Jacketing Wire Types: SEOW; SEW; SJEOW;..
Brittleness Temperature -52.0 °C
-61.6 °F
Type A, type 1 specimen; ASTM D746
Chevron Phillips Marlex® 1003 LDPE Injection Molding Resin
Resin Type: HomopolymerCharacteristics: Excellent flexibilityExcellent flowModerate mold releaseGood warpage resistanceApplications: HousewaresTamper evident, snap-on capsWine bottle sleeve capsInfo..
Brittleness Temperature -52.0 °C
-61.6 °F
Cold Flex; ISO 458/2
Fainplast Compounds GS 55/T Flexible PVC, Injection Molding for Footwear
Soles
Brittleness Temperature -52.0 °C
-61.6 °F
ASTM D746
Colorite Polymers 8088 Non-Phthalate 88 Series Vinyl Compound
Description: The Colorite 88 series is a family of vinyl non-toxic compounds formulated to provide excellent low temperature flexibility characteristics. These compounds are designed for outside doo..
Brittleness Temperature -52.0 °C
-61.6 °F
AlphaGary Smokeguard™ HP 700 High Performance Fluoropolymer
Smokeguard™ HP is a high performance fluoropolymer compound with excellent flame and smoke properties intended for difficult constructions and test requirements
Brittleness Temperature -52.0 °C
-61.6 °F
ASTM D-746
Axiall 18750 Wire & Cable Flexible PVC
Jacketing compound with excellent low temperature performance. Maximum 105°C service temperature at 40+ mil thickness.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in ..
Brittleness Temperature -52.0 °C
-61.6 °F
ASTM D-746
Axiall 18752 Wire & Cable Flexible PVC
Electrical grade extrusion compound with excellent low temperature performance. Maximum service temperature of 105°CInformation provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 20..
Brittleness Temperature -52.0 °C
-61.6 °F
Cold Flex; ISO 458/2
Fainplast Compounds PM 50/C Flexible PVC, Extrusion
Gaskets for frames