Material Notes:
Gaskets for frames
Physical Properties Metric English Comments
Density 1.48 - 1.52 g/cc
0.0535 - 0.0549 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 56 - 60
56 - 60
ISO R 868
Tensile Strength at Break 5.00 MPa
725 psi
ISO R 527
Elongation at Break 320 %
320 %
ISO R 527
Thermal Properties Metric English Comments
Brittleness Temperature -52.0 °C
-61.6 °F
Cold Flex; ISO 458/2