Thermal Properties Metric English Comments
Brittleness Temperature -90.0 - -60.0 °C
-130 - -76.0 °F
Average value: -68.9 °C Grade Count:21
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Butene, Film
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Butene, Film". Each property range of values reported is minimum..
Brittleness Temperature -76.0 - -60.0 °C
-105 - -76.0 °F
Average value: -72.0 °C Grade Count:4
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and..
Brittleness Temperature -73.0 - -60.0 °C
-99.4 - -76.0 °F
Average value: -69.8 °C Grade Count:4
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Compounding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Compounding Grade". Each property range of values reported is minimu..