Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Westlake EMAC® SP1400 Specialty Copolymer
(discontinued **) EMAC resins adhere to and are compatible with a wide range of materials including paper, polyolefins, oriented polyolefins, polyesters, ionomers, PVdC, unplasticized PVC and other polar polymers. Fo.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Westlake EMAC® SP2242 Specialty Copolymer
(discontinued **) EMAC resins adhere to and are compatible with a wide range of materials including paper, polyolefins, oriented polyolefins, polyesters, ionomers, PVdC, unplasticized PVC and other polar polymers. Fo.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Eastman E6837-539A Polyethylene
(discontinued **) PolyethyleneE6837-539A is used in various injection molding applications including closures for containers or extrusion coating for high stiffness. It has good processability. This product may be us.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Eastman E6838-889P Polyethylene
(discontinued **) Polyethylene E6838-889P is a formulation suggested for extrusion coating applications and has been used successfully in compounding. This product may be used for holding food during cooking.Applicat.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Eastman M30033-P Voridian Polyethylene
(discontinued **) VORIDIAN M30033-P polyethylene is suggested for applications such as spiral-wound can linings, release paper and photographic paper. M30033-P has been found to exhibit good barrier properties, tempe.. |
|||
Brittleness Temperature | -73.0 °C | -99.4 °F | ASTM D746 |
Eastman Tenite Polyethylene 1810A Low Density Polyethylene - Molding
(discontinued **) Product Description: TENITE Polyethylene 1810A contains NO ADDITIVES. It is suggested for injection molding applications. TENITE Polyethylene 1810A meets the requirements of FDA regulation 21 CFR 1.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Eastman 1550A Polyethylene
(discontinued **) Injection molding gradeUnless otherwise noted, all tests are run at 23°C and 50% RH. Where required, samples are compression molded per ASTM D1928.Information from manufacturer data sheet.Eastman .. |
|||
Brittleness Temperature | -73.0 °C | -99.4 °F | ASTM D746 |
Eastman 1810E Polyethylene
(discontinued **) Polyethylene 1810E contains no additives. It is suggested for general purpose extrusion applications requiring good stress crack resistance or electrical properties. It is used in applications suc.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Eastman 1830A Polyethylene
(discontinued **) Polyethylene 1830A is a low density formulation. It is suggested for injection molding applications requiring good stiffness or gloss properties . It us used in applications such as closures.Polyet.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Eastman 1830E Polyethylene
(discontinued **) Polyethylene 1830E is a low density formulation. It is suggested for general purpose extrusion applications, such as tubing and blow molding. Polyethylene 1830E meet the requirements of FDA regula.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Eastman 800A Polyethylene
(discontinued **) Polyethylene 800A is a general-purpose low density formulation used for injection molding applications that require good stress-crack resistance. Polyethylene 800E is used in general-purpose extrus.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Eastman 808A Polyethylene
(discontinued **) Low density polyethylene 808A is a general-purpose formulation used for injection molding and general-purpose extrusion.Unless otherwise noted, all tests are run at 23°C and 50% RH.Information from.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Eastman 808P Polyethylene
(discontinued **) Low density polyethylene 808P is a low density resin designed for applications, such as sugar pouches and freezer wrap, where high coating speeds and good drawdown are required. The combination of .. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Eastman M2004-P Polyethylene
(discontinued **) M2004-P polyethylene is suggested for applications such as spiral-wound can linings, release paper and photographic paper. M2004-P has been found to exhibit good barrier properties, temperature res.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
SCG Chemicals EL-Leneâ„¢ LD2305F Low Density Polyethylene Film Key Characteristics:Excellent clarity and glossGood zip formationContains 1000 ppm slip agent and 500 ppm antiblocking agentRecommended Applications:Zip bagsGeneral purpose film for food packagingIn.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Westlake EBAC® Plus SP1903 18% Ethylene Butyl Acrylate Copolymer Westlake EBAC® SP1903 is an 18% EBA copolymer designed for blown film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP1903 provides excel.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Westlake EBAC® SP1806 17.5%, Ethylene-Methyl Acrylate Copolymer Description: Westlake EBAC® SP1806 is an ethylene butyl acrylate copolymer designed for extrusion coating and laminating. SP1806 can also be compounded as an impact modifier or used in highly fill.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Westlake EMAC® Plus SP1305 20% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® Plus SP1305 is a 20% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP1305 is.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Westlake EMAC® Plus SP1358 21.5% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® Plus SP1358 is a 21.5% EMA copolymer containing slip and antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Westlake EMAC® SP2202 21.5% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2202 is a 21.5% EMA copolymer designed for blown film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP2202 provides exce.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Westlake EMAC® SP2205 20% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2205 is a 20% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP2205 provide.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Westlake EMAC® SP2207 20% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2207 is a 20% EMA copolymer designed for extrusion coating, tie-layers, and extrusions where flexibility, compatibility, low heat seal temperatures, or high coefficient of friction.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Westlake EMAC® SP2255 17% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2255 is a 17% EMA copolymer containing slip and antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat s.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Westlake EMAC® SP2258 17% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2258 is a 17% EMA copolymer containing slip and antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat s.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM-D746 |
Westlake EMAC® SP2404 18.5% EMA Copolymer Westlake EMAC� SP2404 is a 18.5% EMA copolymer designed for blown film, tie-layer, coextrusions, and blending where flexibility and strength are important. SP2404 provides excellent elasticity .. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM-D746 |
Westlake EMAC® SP2409 20% EMA Copolymer Westlake EMAC� SP2409 is a 20% EMA copolymer designed for extrusion coating, tie-layers, and extrusions where flexibility, compatibility, low heat seal temperatures, or a high coefficient of fr.. |
|||
Brittleness Temperature | -73.0 °C | -99.4 °F | |
Dow Corning SILASTIC® LCS-740 SILICONE RUBBER 40 Durometer, translucent, low compression set, uncatalysed Silicone Rubber Base suitable for molding.Information provided by Dow Corning |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Westlake EMAC® SP2261 23% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2261 is a 23% EMA copolymer containing antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal tempe.. |
|||
Brittleness Temperature | -73.0 - -60.0 °C | -99.4 - -76.0 °F | Average value: -69.8 °C Grade Count:4 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Compounding Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Compounding Grade". Each property range of values reported is minimu.. |
|||
Brittleness Temperature | -73.0 - -30.0 °C | -99.4 - -22.0 °F | Average value: -62.3 °C Grade Count:4 |
Overview of materials for Ethylene Butyl Acrylate This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Butyl Acrylate". Each property range of values reported is minimum and maximum values of approp.. |