Thermal Properties Metric English Comments
Brittleness Temperature -85.0 - -77.0 °C
-121 - -107 °F
Average value: -82.3 °C Grade Count:3
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade". Each property range of values reported..