Thermal Properties Metric English Comments
Brittleness Temperature -85.0 - -77.0 °C
-121 - -107 °F
Average value: -82.3 °C Grade Count:3
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade". Each property range of values reported..
Brittleness Temperature <= -85.0 °C
<= -121 °F
ASTM D696
NOVA Chemicals Novapol® HB-Y556-A HDPE Extrusion Resin  (discontinued **)
Molded Plaque Properties. Features: Excellent ESCR, high rigidity and impact strength, good melt strength.Applications: chemical bottles, toys, blend for use with post-consumer resins.Data provided..
Brittleness Temperature -85.0 °C
-121 °F
ASTM D746
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with Benzoflex 9-88SG
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Brittleness Temperature -85.0 °C
-121 °F
ASTM D746
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with Butyl Oleate
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Brittleness Temperature -85.0 °C
-121 °F
ASTM D746
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with Benzoflex 9-88SG
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Brittleness Temperature -85.0 °C
-121 °F
ASTM D746
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with Butyl Oleate
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Brittleness Temperature -85.0 °C
-121 °F
ASTM D746
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with Cumar P-10
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Brittleness Temperature <= -85.0 °C
<= -121 °F
ASTM D746
ExxonMobil HDPE BA53-055 High Density Polyethylene Resin
Product Description: BA53-055 is a high molecular weight, high density polyethylene copolymer.Availability: Latin America, North America and South America Additive: Antistatic: NoApplications: Dru..
Brittleness Temperature <= -85.0 °C
<= -121 °F
ASTM D746
ExxonMobil HDPE HYA021L High Density Polyethylene Resin
Product Description: HYA021L is a molecular weight, high-density polyethylene copolymer. This resin has superior stress crack resistance, high impact strength and good rigidity.Availability: Latin A..
Brittleness Temperature -85.0 °C
-121 °F
ASTM D746; ISO 812
Advanced Polymer Alloys Alcryn® 2070 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Brittleness Temperature -85.0 °C
-121 °F
ASTM D746; ISO 812
Advanced Polymer Alloys Alcryn® 2060 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Brittleness Temperature -85.0 °C
-121 °F
ASTM D746
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with Cumar P-10
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Brittleness Temperature -85.0 - 0.000 °C
-121 - 32.0 °F
Average value: -52.5 °C Grade Count:80
Overview of materials for Low Density Polyethylene (LDPE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum ..