Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Brittleness Temperature = -81.0 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Brittleness Temperature -62.8 °C
-81.0 °F
ASTM D746
PolyOne Geon™ Vinyl Wire & Cable JC837DB Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Brittleness Temperature -62.8 °C
-81.0 °F
ASTM D746
ExxonMobil Santoprene® 8221-60 Thermoplastic Rubber  (discontinued **)
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide..
Brittleness Temperature -62.8 °C
-81.0 °F
ASTM D746
ExxonMobil Santoprene® 111-35 Thermoplastic Elastomer
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Brittleness Temperature -62.8 °C
-81.0 °F
ASTM D746
ExxonMobil Santoprene® 121-55W241 Thermoplastic Elastomer
A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in difficult ..
Brittleness Temperature -62.8 °C
-81.0 °F
ASTM D746
ExxonMobil Santoprene® 8201-80 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w..
Brittleness Temperature -62.8 °C
-81.0 °F
ASTM D746
ExxonMobil Santoprene® 8211-65 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif..
Brittleness Temperature -62.8 °C
-81.0 °F
ASTM D746
ExxonMobil Santoprene® 8271-55 Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated ..
Brittleness Temperature -62.8 °C
-81.0 °F
ASTM D746
ExxonMobil Santoprene® 8271-65 Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated ..
Brittleness Temperature -62.8 °C
-81.0 °F
ASTM D746
ExxonMobil Santoprene® 8211-60 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, non-hygroscopic, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance ..