Material Notes:
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range of applications. This grade of Santoprene 8000 TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding, extrusion or blow molding. It is polyolefin based and completely recyclable.Key Features: Non-hygroscopic product, requires little to no drying before processing.Neutral, easy coloring formulation.Recommended for applications requiring excellent ozone resistance.Used in sealing applications.Recommended for applications requiring excellent flex fatigue resistance. Although not NSF certified, this product has a Material Supplier Form on file with NSF to facilitate its evaluation for use in applications requiring NSF certification.EU and China RoHS compliantApplications:Consumer – Cell Phones and PackagingGeneral PurposeUses:Appliance ComponentsCell PhonesFlexible GripsKitchenwareStationary SuppliesStrain ReliefsProcessing Method: Blow Molding, Coextrusion, Extrusion, Extrusion Blow Molding, Injection Molding, Multi Injection Molding, Profile Extrusion, Sheet Extrusion, Thermoforming and Vacuum FormingAvailability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
2 mm, 15 sec; ISO 868
86
86
Air at 302°F, 168 hr; ASTM D573
Tensile Strength at Break 9.2031 MPa
1334.8 psi
Air at 302°F, 168 hr; ASTM D573
9.79 MPa
1420 psi
Across Flow; ASTM D412
Elongation at Break 510.3 %
510.3 %
Air at 302°F, 168 hr; ASTM D573
630 %
630 %
Across Flow; ASTM D412
Tear Strength 43.1 kN/m
246 pli
73°C, Die C; ASTM D624
Compression Set 35 %
35 %
158°F, 22 hr; ASTM D395
69 %
69 %
257°F, 70 hr; ASTM D395
Thermal Properties Metric English Comments
Brittleness Temperature -62.8 °C
-81.0 °F
ASTM D746
UL RTI, Electrical 100 °C
212 °F
UL 746
UL RTI, Mechanical with Impact 90.0 °C

@Thickness 27.9 mm
194 °F

@Thickness 1.10 in
UL 746
90.0 °C

@Thickness 40.6 mm
194 °F

@Thickness 1.60 in
UL 746
95.0 °C

@Thickness 76.2 mm
203 °F

@Thickness 3.00 in
UL 746
Flammability, UL94 HB

@Thickness 27.9 mm
HB

@Thickness 1.10 in
HB

@Thickness 40.6 mm
HB

@Thickness 1.60 in
HB

@Thickness 76.2 mm
HB

@Thickness 3.00 in
Electrical Properties Metric English Comments
Volume Resistivity 2.40e+16 ohm-cm
2.40e+16 ohm-cm
3.30 mm; ASTM D257
5.50e+17 ohm-cm
5.50e+17 ohm-cm
2.03 mm; ASTM D257
Processing Properties Metric English Comments
Processing Temperature 175 - 230 °C
347 - 446 °F
Rear Barrel Temperature 185 - 199 °C
365 - 390 °F
Middle Barrel Temperature 191 - 204 °C
375 - 400 °F
Front Barrel Temperature 191 - 204 °C
375 - 400 °F
Nozzle Temperature 199 - 216 °C
390 - 420 °F
Die Temperature 191 - 224 °C
375 - 435 °F
Extrusion
Melt Temperature 199 - 216 °C
390 - 420 °F
Processing
191 - 224 °C
375 - 435 °F
Extrusion
Mold Temperature 23.9 - 51.7 °C
75.0 - 125 °F
Processing
Moisture Content 0.080 %
0.080 %
Back Pressure 0.345 - 0.689 MPa
50.0 - 100 psi
Clamp Pressure 41.4 - 68.9 MPa
6000 - 10000 psi
Vent Depth 0.00254 cm
0.00100 in
Cushion 0.317 - 0.635 cm
0.125 - 0.250 in
Screw Speed 100 - 200 rpm
100 - 200 rpm
Descriptive Properties Value Comments
Change in Mass in Air -8.0%
150°C, 168 hr, ASTM D573
Color Natural Color
Form Pellets
Injection Rate Fast
Maximum Regrind % 20
Screw Compression Ratio 2:1 - 2.5:1
Screw L/D Ratio 16:1 - 20:1