Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -76.0 - 20.0 °C | -105 - 68.0 °F | Average value: -69.6 °C Grade Count:15 |
Overview of materials for ECTFE Fluoropolymer This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat.. |