Polymer Property : Deflection Temperature at 8.0 MPa = 127 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 8.0 MPa 53.0 °C
127 °F
ISO 75-1/-2
Lanxess Durethan® AC 30 000000 Nylon 66
PA 66, injection molding-grade, non-reinforced, higher notched impact strength than A 30 / A 31 in the dry and conditioned stateApplication Examples: plug connectors, cable binders, cable clips, par..