Thermal Properties Metric English Comments
Deflection Temperature at 8.0 MPa 55.0 °C
131 °F
ISO 75-1/-2
Lanxess Durethan® A 30 S 000000 Nylon 66
PA 66 standard injection molding-grade, non-reinforced, good demolding, very rapid solidificationApplication Examples: plug connectors, terminal blocks, cable clips, bobbins
Deflection Temperature at 8.0 MPa 55.0 °C
131 °F
ISO 75-1/-2
Lanxess Durethan® BKV 15 G H2.0 900051 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers, better surface resistance to alcoholic calcium chloride-solution than BKV 15 H2.0, good heat-ageing resistance
Deflection Temperature at 8.0 MPa 55.0 °C
131 °F
ISO 75-1/-2
Lanxess Durethan® BKV 315 Z H2.0 901510 Nylon 6, 15% Glass Fiber
PA 6 extrusion- and blow molding-grade with 15% glass fibers, branched/structural viscosity, elastomer-modified, good heat-ageing resistance, dry-impact modifiedApplication Examples: air intake hose..
Deflection Temperature at 8.0 MPa 55.0 °C
131 °F
ISO 75-1/-2
Lanxess Pocan® B 3215 901510 PBT, 10% Glass Fiber
PBT, 10% glass fibers, injection molding
Deflection Temperature at 8.0 MPa 55.0 °C
131 °F
ISO 75-1/-2
EMS-Grivory Grivory® B 70 GFE 15 H PA6-GF15
Product description: Grilon B 70 GFE 15 H is a impact modified, heat stabilized PA 6 injection molding grade with 15% glass fiber reinforcement. Grilon B 70 GFE 15 H has the following important prop..
Deflection Temperature at 8.0 MPa 55.0 °C
131 °F
ISO 75-1/-2
EMS-Grivory Grivory® XE 5052 (BGZ-15 FC) PA6-GF15
Product description: Grilon XE 5052 is a impact modified, heat stabilized PA 6 injection molding grade with 15% glass fiber: High impact resistanceGood surface qualityShort cycle timeGood flowabilit..
Deflection Temperature at 8.0 MPa 55.0 - 190 °C
131 - 374 °F
Average value: 142 °C Grade Count:5
Overview of materials for Nylon 6, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro..
Deflection Temperature at 8.0 MPa 55.0 °C
131 °F
ISO 75-1/-2
Lanxess Pocan® B 3215 000000 PBT, 10% Glass Fiber
PBT, 10% glass fibers, injection molding
Deflection Temperature at 8.0 MPa 55.0 °C
131 °F
ISO 75-1/-2
EMS-Grivory Grivory® BGZ-15/2 PA6-GF15
Product description: Grilon BGZ-15/2 is a heat stabilized and impact modified PA6 injection molding grade with 15% glass fibers. Grilon BGZ-15/2 has the following important properties: Good impact s..