Material Notes:
Product description: Grilon XE 5052 is a impact modified, heat stabilized PA 6 injection molding grade with 15% glass fiber: High impact resistanceGood surface qualityShort cycle timeGood flowabilityGood processability Application examples are parts with critical wall thickness-flow length ratio like housings or functional parts in automotive with high demands to the impact strength.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ISO 1183
Water Absorption 8.0 %
8.0 %
ISO 62
Moisture Absorption 2.00 %
2.00 %
ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.0 MPa
9430 psi
conditioned; ISO 527-1/-2
110 MPa
16000 psi
dry; ISO 527-1/-2
Elongation at Break 5.0 %
5.0 %
dry; ISO 527-1/-2
15 %
15 %
conditioned; ISO 527-1/-2
Tensile Modulus 2.80 GPa
406 ksi
conditioned; ISO 527-1/-2
5.30 GPa
769 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 7.50 J/cm²
35.7 ft-lb/in²
dry; ISO 179/1eU
9.00 J/cm²
42.8 ft-lb/in²
conditioned; ISO 179/1eU
7.00 J/cm²

@Temperature 30.0 °C
33.3 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
7.50 J/cm²

@Temperature 30.0 °C
35.7 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
dry; ISO 179/1eA
2.50 J/cm²
11.9 ft-lb/in²
conditioned; ISO 179/1eA
1.10 J/cm²

@Temperature 30.0 °C
5.23 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
1.20 J/cm²

@Temperature 30.0 °C
5.71 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 50.0 µm/m-°C
27.8 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
Melting Point 222 °C
432 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 120 °C
194 - 248 °F
long term; EMS
160 °C
320 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 190 °C
374 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 55.0 °C
131 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
1.00e+14 ohm-cm
1.00e+14 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 35.0 kV/mm
889 kV/in
conditioned; IEC 60243-1
40.0 kV/mm
1020 kV/in
dry; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Automotive electr. and electronics, lighting
Interior
Powertrain and Chassis
Electricals & Electronics Connectors
Electrical appliances
Electrical equipment
Form Granules
Industry & Consumer goods Housewares
Mechanical Engineering
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Product Attributes Improved flowability and demoulding
Special Characteristics High impact or impact modified
Users viewing this material also viewed the following: