Thermal Properties Metric English Comments
Deflection Temperature at 8.0 MPa 205 °C
401 °F
ISO 75-1/-2
Lanxess Durethan® AKV 50 H2.0 901510 Nylon 66, 50% Glass Fiber
PA 66, injection molding grade, 50% glass fibers, good heat-ageing resistance
Deflection Temperature at 8.0 MPa 205 °C
401 °F
ISO 75-1/-2
EMS-Grivory Grivory® HTV-45H1 black 9205 PA6T/6I-GF45
Product description: Grivory HTV-45H1 black 9205 is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation a..
Deflection Temperature at 8.0 MPa 205 °C
401 °F
ISO 75-1/-2
EMS-Grivory Grivory® GVX-6 H black 9915 PA*-GF60
Product description: Grivory GVX-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam..
Deflection Temperature at 8.0 MPa 205 °C
401 °F
ISO 75-1/-2
EMS-Grivory Grivory® GVX-6 H nat PA*-GF60
Product description: Grivory GVX-6H natural is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamid..
Deflection Temperature at 8.0 MPa 205 °C
401 °F
ISO 75-1/-2
EMS-Grivory Grivory® HT1V-45 HY black 9205 PA6T/6I-GF45
Product description: Grivory HT1V-45 HY black 9205 is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-45 HY ..
Deflection Temperature at 8.0 MPa 205 °C
401 °F
HDT/C; ISO 75-1/2
Akro-Plastic Akromid® T1 GF 50 9 (3257) PPA Dry, 50% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
Deflection Temperature at 8.0 MPa 205 °C
401 °F
HDT/C; ISO 75-2
Akro-Plastic Akromid® T1 GF 40 (3464) PPA Dry, 40% Glass Filled