Deflection Temperature at 1.8 MPa (264 psi) 90.0 - 100 °C
194 - 212 °F
ASTM D648
Plaskolite Optix® CA-81 UVA UV-Absorbing Acrylic Resin
Special UV-absorption grade, extrusion and injection moldingApplications: A special UV-absorption acrylic resin for extrusion and injection molding. It is slightly lubricated for ease of processing..
Deflection Temperature at 1.8 MPa (264 psi) 90.0 - 100 °C
194 - 212 °F
ASTM D648
Plaskolite West Optix® CA-81 UVA UV-Absorbing Acrylic Resin
Special UV-absorption grade, extrusion and injection moldingApplications: A special UV-absorption acrylic resin for extrusion and injection molding. It is slightly lubricated for ease of processing..
Deflection Temperature at 1.8 MPa (264 psi) 90.0 - 100 °C
194 - 212 °F
ASTM D648
Plaskolite West Optix® CA-81 UVA-7 UV-Absorbing Acrylic Resin
Special UV-absorption grade, extrusion and injection moldingApplications: A special UV-absorption acrylic resin for extrusion and injection molding. It is slightly lubricated for ease of processing..