Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 90.0 - 100 °C | 194 - 212 °F | ASTM D648 |
Plaskolite Optix® CA-81 UVA UV-Absorbing Acrylic Resin Special UV-absorption grade, extrusion and injection moldingApplications: A special UV-absorption acrylic resin for extrusion and injection molding. It is slightly lubricated for ease of processing.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.0 - 100 °C | 194 - 212 °F | ASTM D648 |
Plaskolite West Optix® CA-81 UVA UV-Absorbing Acrylic Resin Special UV-absorption grade, extrusion and injection moldingApplications: A special UV-absorption acrylic resin for extrusion and injection molding. It is slightly lubricated for ease of processing.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.0 - 100 °C | 194 - 212 °F | ASTM D648 |
Plaskolite West Optix® CA-81 UVA-7 UV-Absorbing Acrylic Resin Special UV-absorption grade, extrusion and injection moldingApplications: A special UV-absorption acrylic resin for extrusion and injection molding. It is slightly lubricated for ease of processing.. |