Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 69.0 - 73.0 °C | 156 - 163 °F | ASTM D648 |
Reliance Industries PVAXX H65 The key property of all PVAXX polymer is this product`s unique capacity to biodegrade into non-toxic residues under both aerobic and non-aerobic conditions.Information provided by Reliance Industrie.. |